Title: Some Features of the Testing of Stevenson Creek Arch Dam

Author(s): Willis A. Slater

Publication: Journal Proceedings

Volume: 24

Issue: 2

Appears on pages(s): 273-301

Keywords: none

Date: 2/1/1928

Abstract:
In the fall of 1925 the Bureau of Standards was called upon by Engineering Foundation for advice relative to the construction ant1 for assistance in the testing of a concrete arch dam in California which was to be built and tested by Engineering Foundation Committee on Arch Dam Investigation.




  