ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: SP-179: Fourth CANMET/ACI/JCI Conference: Advances in Concrete Technology

Author(s): Editor: V.M. Malhotra

Publication: Symposium Paper

Volume: 179

Issue:

Appears on pages(s): 1109

Keywords:

DOI: 10.14359/14172

Date: 6/1/1998

Abstract:
This Symposium Publication contains the proceedings of the Fourth CANMET/ACI/JCI International Conference held in Tokushima, Japan, in June 1998. Sixty-two refereed papers were accepted for presentation at this conference and for this publication. Note: The individual papers are also available as .pdf downloads.. Please click on the following link to view the papers available, or call 248.848.3800 to order. SP179




  

Please enter this 5 digit unlock code on the web page.