Title: SP-064: Cedric Willson Symposium on Expansive Cement

Author(s): Editor: William P. Liljestrom

Publication: Symposium Paper

Volume: 64

Issue:

Appears on pages(s): 336

Keywords:

Date: 7/1/1980

Abstract:
SP-64 This symposium of 16 papers covers international developments, field service reports on existing installations and research. Reports on applications of shrinkage-compensating concrete in hydraulic structures, cold storage warehouse, slabs, bridge decks, oil well cementing, post-tensioned structures.




  