Title: SP-009: Symposium on Creep of Concrete

Author(s): Editor: A.M. Neville

Publication: Symposium Paper

Volume: 9

Issue:

Appears on pages(s): 160

Keywords:

Date: 1/1/1964

Abstract:
SP9 A compilation of 6 papers giving a state-of-the-art report on various aspects of creep in concrete, written by authorities in this field and supported by formal discussion.




  