Title: SP-089: Polymer Concrete: Uses, Materials and Properties
Author(s): Editors: James T. Dikeou and David W. Fowler
Publication: Symposium Paper
Volume: 89
Issue:
Appears on pages(s): 346
Keywords:
Date: 12/1/1985
Abstract:
SP-89
A collection of 17 papers dealing exclusively with the various effects of polymers in concrete, this book provides an extensive source of reference material. Presents advances in research, development, and uses of polymers. Case studies cover the effect of moisture on the physical and durability properties of methyl methacrylate polymer concrete; machine application of polymer concrete for highway repairs, commercial applications of epoxies in construction, and polymer concrete for bridge rehabilitation.