Title: Petrographic Examination of Mortar Coatings--0 to 60-Year-Old Water Pressure Pipes

Author(s): Lars Palbøl, Ulla Hjorth Jakobsen, and Niels Thaulow

Publication: Concrete International

Volume: 20

Issue: 3

Appears on pages(s): 47-52

Keywords: carbonation; corrosion; durability; hydration; petrography; pipes (tubes); porosity; protective coatings; water-cement ratio;

DOI:

Date: 3/1/1998

Abstract:
This article presents the results of petrographic examination of currently manufactured and older in-service mortar coatings. Based on analyses of 11 mortar samples from pipe of varying ages (0 to 60 years old), the mortar samples were evaluated for durability to withstand corrosion. The analyses demonstrated that the mortar coating samples taken from in-service concrete pressure pipes of varying ages displayed excellent durability. All coatings provided effective corrosion protection for the steel elements of the pipe. Furthermore, recent improvements to the mortar coatings should offer even better protection.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer