Experimental Aids in Structural Concrete Design

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Aids in Structural Concrete Design

Author(s): R. E. Glover, O.J. Olsen and Carl Zangar

Publication: Journal Proceedings

Volume: 45

Issue: 2

Appears on pages(s): 445-466

Keywords: no keywords

DOI: 10.14359/12154

Date: 2/1/1949

Abstract:
Statically determinate and inderminate structures are generally designed by analytical methods. This paper describes several experimental aids which have been used in the design and stress analysis of statically indeterminate structures at the laboratories of the Bureau of Reclamation. These methods are used where analytical procedures cannot be conviently be applied. Described herein are photoelastic methods using both the polariscope and interferometer, the Beggs Deformeter, Stresscoat and electric SR-4 Strain gages. Applications are given for each method.