Title: 
            Prestressed Concrete Construction Procedures
        
        
            Author(s): 
            Thor Germundsson
        
        
            
                Publication: 
                Journal Proceedings
            
            
                Volume: 
                46
            
            
                Issue: 
                6
            
            
                Appears on pages(s): 
                857-875
            
            
                Keywords: 
                no keywords
            
            
                DOI: 
                10.14359/12101
            
        
        
            Date: 
            6/1/1950
        
        
            Abstract:
            In reviewing the construction procedures used in the production of prestressed concrete, the methods of prestressing are grouped under several simple classifications.  A brief outline of these methods is presented, and typical prestressing procedures are described and illustrated.