ACI Standard Recommended Practice for the Application of Mortar by Pneumatic Pressure (ACI 805-51)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI Standard Recommended Practice for the Application of Mortar by Pneumatic Pressure (ACI 805-51)

Author(s): ACI Committee 805

Publication: Journal Proceedings

Volume: 47

Issue: 5

Appears on pages(s): 709-719

Keywords: no keywords

DOI: 10.14359/12031

Date: 5/1/1951

Abstract:
This ACI Standard presents briefly the advantages and disadvantages of pnuematically-placed mortar and establshed recommended practices for placing and mixing shotcrete, qualifications and duties of workmen, preparation of surface before shotcreteing, reinforcing, sequence of application, and other items involved in good shotcreting.




  