Title: Application of Vibration to Concrete Pavement Construction
Author(s): A. G. Timms
Publication: Journal Proceedings
Volume: 49
Issue: 6
Appears on pages(s): 933-942
Keywords: no keywords
Date: 6/1/1953
Abstract:
Brief description and summary of tests and experience in the United States and Europe in vibrating pavement concrete. Effect of vibration on tolerances in composition of the fresh concrete, gradation of coarse aggregate, and maintaining line and grade of forms are factors in the development of adaquate vibration equipment.