Title: Investigation of Stud Shear Connectors for Composite Concrete and Steel T-Beams

Author(s): I. M. Viest

Publication: Journal Proceedings

Volume: 52

Issue: 4

Appears on pages(s): 875-892

Keywords: no keywords

DOI: 10.14359/11655

Date: 4/1/1956

Abstract:
Push-out tests of round steel studs were made to determine the behavior and load carrying capacity of stud shear connectors. The tests have shown that a steel stud is suitable for use as a shear connector in composite concrete and steel construction. Empirical equations are presented for determining critical load.