Title: Proposed ACI Standard 503.2: Standard Specification for Bonding Plastic Concrete to Hardend Concrete with a Multi-Component Epoxy Adhesive
Author(s): ACI Committee 503
Publication: Journal Proceedings
Volume: 75
Issue: 9
Appears on pages(s): 442-447
Keywords: adhesives;bond (concrete to concrete);bonding;concrete construction;epoxy resins;fresh concretes;hardened concrete;quality control;repairs;specifications; standards.
Date: 9/1/1978
Abstract:
This specification describes the work of bonding plastic concrete to hardend concrete with a multi-compnenet epoxy adhesive such as defined for this purpose in ASTM C881. It includes controls for adhesive labeling, storage, handling, mixing and application, surface evaluation and preparation, as well as inspection and quality conrol.