Title: Mixture Proportioning for Durable Concrete: Challenges and Changes

Author(s): S. P. Shah, K. Wang, and W. J. Weiss

Publication: Concrete International

Volume: 22

Issue: 9

Appears on pages(s): 73-78

Keywords:

DOI:

Date: 9/1/2000

Abstract:
Numerous changes and innovations have occurred in concrete materials and technology during the last century. These changes have provided engineers with many advantages in design and construction of concrete structures. At the same time, however, the application of the new developments and changes in concrete mixture proportions have also generated new durability problems.




  