Effect of Corner Angle on Efficiency of Reinforced Concrete Joints under Opening Bending Moment

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Corner Angle on Efficiency of Reinforced Concrete Joints under Opening Bending Moment

Author(s): Hashim M. S. Abdul-Wahab and Shamil A. R. Salman

Publication: Structural Journal

Volume: 96

Issue: 1

Appears on pages(s): 115-121

Keywords: corner joints; diagonal tension; efficiency; experimental study; opening bending moment; reinforced concrete; ultimate strength

DOI: 10.14359/602

Date: 1/1/1999

Abstract:
Results of an experimental investigation of the effect of the corner angle on the strength and behavior of reinforced concrete corners under opening bending moments are presented. Twelve specimens divided into two groups with two reinforcement details and the included angle varying from 60 to 180 deg were tested. From the results obtained, and from those reported by others, it was found that the efficiency of the joint is significantly affected by the angle and is at its minimum when at 120 deg. Theoretical analysis using finite element method (FEM) confirms the same variation of the diagonal tensile stress concentration with the angle.


ALSO AVAILABLE IN:

Electronic Structural Journal