Title: Behavior of Concrete Under Triaxial Compressive-Compressive-Tensile Stresses

Author(s): Jiang Linhua, Huang Dahai, and Xie Nianxiang

Publication: Materials Journal

Volume: 88

Issue: 2

Appears on pages(s): 181-185

Keywords: compressive strength; concretes; stress-strain relationship; tensile strength; tests; triaxial stresses; Materials Research

DOI: 10.14359/1982

Date: 3/1/1991

Abstract:
Seventy-nine 10 x 10 x 55-cm prisms for triaxial compression-compression-tension specimens were tested. The tests were taken in a special device containing two compression testing apparati to exert lateral compressive loadings and an ordinary universal material-testing machine to exert longitudinal tensile loading. One 3 mm fluorine-based resin sheet was used as a friction-reducing pad. Test results of strength and stress-strain relationships were analyzed and formulas of concrete strength are suggested. Failure modes of specimens are also described.