Influence of Aggregate Surface Area on Mechanical Properties of Mortar

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Aggregate Surface Area on Mechanical Properties of Mortar

Author(s): Christine Float Goble and Menashi D. Cohen

Publication: Materials Journal

Volume: 96

Issue: 6

Appears on pages(s): 657-662

Keywords: aggregates; silica fume; strain energy methods; strains; stresses.

DOI: 10.14359/791

Date: 11/1/1999

Abstract:
Mortar mixtures containing various aggregate surface areas were tested in compression in an effort to quantify the mechanical effects of the transition zone (between the cement paste and aggregate). Special consideration was taken to establish a testing program, which would generate the complete stress-strain curve, including the strain-softening region. The assumption is made that the transition zone is of constant thickness regardless of aggregate size; therefore, increasing aggregate surface area increases the percentage of the transition zone in the mortar. Mortar strength was found to increase as the quantity of transition zone material was increased. Silica fume (SF) was incorporated into a series of mixtures and found to modify the transition zone and, therefore, the stress-strain behavior of the mortar.


ALSO AVAILABLE IN:

Electronic Materials Journal