Author(s):

Sam Slatnick, Kyle A. Riding, Kevin J. Folliard, Maria C. G. Juenger, and Anton K. Schindler

Publication:

Materials Journal

Volume:

108

Issue:

1

Abstract:

Autogenous shrinkage, significant primarily in concretes with a low water-cementitious material ratio (w/cm), has received more attention in recent years due to the increasing use of high-performance concretes (HPCs). In this study, autogenous shrinkage was quantified in both unrestrained and restrained concrete. The specimens were sealed and kept at a constant isothermal temperature of 20°C (68°F) to prevent deformation due to temperature change or moisture loss. Various materials were evaluated to compare their effectiveness in reducing autogenous deformation and stress development, including saturated lightweight aggregates, shrinkage-reducing admixtures (SRAs), and a shrinkage-compensating additive (based on calcium sulfoaluminate). The data obtained also provide insight into the mechanisms behind autogenous shrinkage and the resulting stress development in restrained members and quantify the effects of methods used to reduce autogenous shrinkage and the resultant stresses.

DOI:

10.14359/51664212


Document: 

104-M69

Date: 

November 1, 2007

Author(s):

Michael D. Brown, Cuyler A. Smith, J. Greg Sellers, Kevin J. Folliard, and John E. Breen

Publication:

Materials Journal

Volume:

104

Issue:

6

Abstract:

According to a survey conducted in 1996, respondents in several state departments of transportation indicated that more than 100,000 bridge decks in the U.S. have suffered from early age transverse cracking, a crack pattern that typically arises due to drying shrinkage. Concrete material properties are treated as a means through which to improve the resistance restrained drying shrinkage cracking. Various test methods are discussed as they relate to determining the resistance of a material to shrinkage cracking. Materials-based methods of controlling drying shrinkage are presented. The materials discussed include fibers, shrinkage-compensating concrete, shrinkage-reducing admixtures, and extensible concrete. It was determined in small laboratory specimens, and confirmed in large-scale bridge deck specimens, that several of the alternative mixtures adequately reduced restrained drying-shrinkage cracking.

DOI:

10.14359/18967


Document: 

88-M59

Date: 

September 1, 1991

Author(s):

Jan Olek and Menashi D. Cohen

Publication:

Materials Journal

Volume:

88

Issue:

5

Abstract:

Paper presents a procedure for mix proportioning of Type K expansive cement blends for use in shrinkage-compensating mortars. The proposed procedure is based on a simple linear regression model correlating maximum expansion in Type K expansive cement mortars with expansion time (duration) of mortar and composition of expansive cement ingredients. The model provides a practical means of correlating such parameters as the composition and relative proportions of expansive cement mortar ingredients with the duration of curing so that the resulting mortar can satisfy expansion criteria specified in ASTM C 806. The model demonstrates that, for the range of parameters and materials used in this investigation, there is a reasonable correlation between the square root of expansion, the mass of expansive component in the expansive cement blend, and the expansion time. Furthermore, the mass of the expansive component does not appear to be an exclusive and reliable predictor of the amount of expansion strain. The expansion time must be considered as well in the overall relationship.

DOI:

10.14359/2203


Results Per Page 




Please enter this 5 digit unlock code on the web page.