ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Showing 1-5 of 10880 Abstracts search results
Document:
CI4708UlmerTechSpotlight
Date:
August 1, 2025
Author(s):
Seth Ulmer
Publication:
Concrete International
Volume:
47
Issue:
8
Abstract:
Traditional placements often require curb and gutter work to be placed, finished, and cured to outline the pavement area before completion of the flatwork. Monolithic placements, or all-in-one placements, improve efficiency by completing the curb and gutter at the same time as the flatwork. Curbing machines with multiple drum options are the proper tools for such placements.
CI4708White
Chad White, Bryan M. Birdwell, Jerry A. Holland, and Michael G. Hernandez
This article discusses differences between ordinary portland cement (Type I/II) and portland-limestone cement (Type IL) concrete based on direct observations and reports from concrete finishers. Developing an understanding of how these two concrete types differ from each other can help contractors modify and adapt finishing practices to avoid possible issues during placement.
CI4708BrownTechSpotlight
Daron Brown
Internally cured concrete was used to repair bridge decks of the Wilson Dam in Muscle Shoals, AL, USA, and to provide a 100-year service life. The article discusses characteristics of internally cured concrete and the benefits of using it, as well as lightweight aggregates needed to produce such concrete and their properties.
CI4708NEUnews
NEU: An ACI Center of Excellence for Carbon Neutral Concrete introduces a new resource, The Low-Carbon Concrete Guide: Materials, that explains how the use of low-carbon materials can help reduce the carbon footprint of concrete. NEU also spotlights Affiliate Member Lyten, Inc., a supermaterials application company.
CI4708Nexinsights
NEx: An ACI Center of Excellence for Nonmetallic Building Materials spotlights the member companies that power their mission. Each organization brings unique expertise, global influence, and an uncompromising commitment to sustainable infrastructure.