Factors Influencing Dry-Process Accelerated Shotcrete
Author(s):
Raymond J. Schutz
Publication:
Concrete International
Volume:
3
Issue:
1
Appears on pages(s):
75-79
Keywords:
accelerating agents; admixtures; com-pressive
strength; flexural strength; hydration; setting
(hardening); shotcrete; voids; water-cement ratio.
DOI:
Date:
1/1/1981
Abstract:
There are many factors influencing accelerated dry process shotcrete. This paper covers the effects of temperatures, admixture, cement composition, prehydration, voids, and water-cement ratio on dry-process shotcrete setting time and strength.