International Concrete Abstracts Portal

  


Title: Discrepancies Between the Volume of Fresh Concrete at the Ready-Mix Plant and the Volume in Final Placement

Author(s): Herbert J. Knopel

Publication: Journal Proceedings

Volume: 37

Issue:

Appears on pages(s): 649-656

Keywords: none

DOI: 10.14359/8579

Date: 6/1/1941

Abstract:
Rapid growth of the ready-mixed concrete industry has entailed production and service *problems. These include technical problems of preclslon control. Ab- solute volume method for deducing resulting yield of wet mixes is sound. Wet mass is altered by evaporation losses, by densification due to agitation, and by bleed- ing throu h forms or subgrades, these varying with degree of manipulation. Purpose of this paper IS t o show where these losses may occur.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.