Mass Concrete Research For Hoover Dam

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mass Concrete Research For Hoover Dam

Author(s): Byram W. Steele

Publication: Journal Proceedings

Volume: 29

Issue:

Appears on pages(s): 305-317

Keywords: none

DOI: 10.14359/8275

Date: 3/1/1933

Abstract:
The advent of a mass concrete dam 726 ft high necessitated a thorough investigation of such subjects as volume change, foundation and contraction joint grouting, portland cement, mass concrete strength and mix proportions, elastic and thermal properties of mass concrete, permeability, precooling concrete ingredients versus concrete re-frigeration, action under axial, biaxial and trlaxlal loads, bond and sliding friction, shear, uplift, and durability. Of these problems, the ones of most vital importance from the construction standpoint were attacked first and solutions obtained that justi-fied the procedure actually followed.