A Study Of Slump And Flow Of Concrete
Author(s):
Inge Lyse and W. R. Johnson
Publication:
Journal Proceedings
Volume:
27
Issue:
1
Appears on pages(s):
439-467
Keywords:
none
DOI:
10.14359/8195
Date:
1/1/1931
Abstract:
An investigation of the relationship between the slump and flow. of concrete showed that the slump gave a more suitable indication than the flow. of the increased workability of concrete produced either by enriching the mix or additions of admixtures. The relation between the flow and the slump changed with the richness of the concrete mix.