Concrete for the Mammoth Pool Power Tunnel

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete for the Mammoth Pool Power Tunnel

Author(s): Neville S. Long and Thomas W. Howell

Publication: Journal Proceedings

Volume: 57

Issue: 5

Appears on pages(s): 1441-1458

Keywords: none

DOI: 10.14359/8071

Date: 5/1/1961

Abstract:
Construction of the Mammoth Pool Power Tunnel provided an excellent opportunity for obtaining concrete at a minimum cost with maximum use of local materials. The combination of an owner operated aggregate plant and a cooperative contractor made possible the achievement of minimum cost concrete. Satisfactory 2000 psi concrete in the tunnel invert was produced from crushed aggregate using as little as 325 lb of cement per cu yd.




  

Edit Module Settings to define Page Content Reviewer