Title: Responsibility in Concrete

Author(s): Roger H. Corbetta

Publication: Journal Proceedings

Volume: 61

Issue: 5

Appears on pages(s): 481-486

Keywords:

DOI: 10.14359/7792

Date: 5/1/1964

Abstract:
Stresses the important role that ACI can play to insure greater quality workmanship in concrete construction. Suggests that a governing body be established with the authority to issue and revoke certificates of competency among con-tractors, concrete suppliers,and testing laboratories.