The Mechanical Properties of Polymer Modified OPC/PFA Pastes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Mechanical Properties of Polymer Modified OPC/PFA Pastes

Author(s): H. Olmez, D. Dollimore, G.A. Gamlen, and R.J. Mangabhai

Publication: Symposium Paper

Volume: 79

Issue:

Appears on pages(s): 607-624

Keywords: blended cements; cement pastes; compressive strength; -- flexural strength; fly ash; heat of hydration; plastics, polymers, -- and resins. --

DOI: 10.14359/6714

Date: 5/1/1983

Abstract:
Investigations have been carried out on the modification of OPC/PFA paste with various polymeric materials, such as Versicol W13, sodium carboxy methyl cellulose, Versicol KA21 and Crodafix. The hardened OPC/PFA pastes were cured under water and their mechanical properties determined. A conduction calorimeter was used to evaluate the heat evolution pattern of the modified paste. The results show that sodium carboxy methyl cellulose and Versicol KA21 act as strong retarders whilst the other two polymers produce only slight retardation. The investigation has been extended to include the ageing effect of the polymers on the mechanical properties of the cement paste and the consequences of these further studies are discussed in detail.




  