Influence of Superheated Steam on the Autoclave-Cure Strengths of Cement and Concrete Compositions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Superheated Steam on the Autoclave-Cure Strengths of Cement and Concrete Compositions

Author(s): W. V. Friedlaender and F. V. Camarda

Publication: Symposium Paper

Volume: 32

Issue:

Appears on pages(s): 99-116

Keywords: asbestos-cement products; au toclaving; compressive strength; concrete blocks; concretes; curing; flexural strength; high temperature; hydration; mortars (material); research; superheated steam.

DOI: 10.14359/6601

Date: 7/1/1972

Abstract:
The influences of superheated steam on the strengths of autoclave cured cement mortar specimens and asbestos-cement compositions were examined. The test results show that superheated steam, apparently because it acts as a desiccant, generally causes reduced strengths that can be related to functions of the cured weight after autoclaving as well as a factor involvinggthe length and degrees of superheat. If super-heated steam is present during the early stages of the curing cycle it causes greater adverse strength effects.




  