Shear and Punching Capacity Predictions for Slabs under Concentrated Loads Aided by LEFEA

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear and Punching Capacity Predictions for Slabs under Concentrated Loads Aided by LEFEA

Author(s): Alex de Sousa, Eva Lantsoght, Andri Setiawan, and Mounir El Debs

Publication: Symposium Paper

Volume: 357

Issue:

Appears on pages(s): 100-122

Keywords: critical shear crack theory, linear elastic finite element analyses, one-way shear, punching shear

DOI: 10.14359/51738762

Date: 4/1/2023

Abstract:
One-way slabs under concentrated loads may fail by one-way shear, punching, flexure or a mixed-mode be-tween them. This study examines the benefits of using Linear Elastic Finite Element Analyses (LEFEA) combined with analytical expressions to predict the shear and punching capacities of such slabs. Besides, the determination of the most critical shear failure mechanism is also addressed. A simplified approach is proposed to predict the shear and punching capacity without numerical models. Forty-eight tests of simply supported slabs under concentrated loads were evaluated. The LEFEA was conducted with ABAQUS. The analytical expressions are based on the Critical Shear Crack Theory (CSCT). The coupling of the CSCT-expressions with the LEFEA accurately predicts the governing shear failure mechanism and the shear capacity of most test results. In this study, it was also found that the punching capacity predictions may be improved by considering the influence of the slab width and load size on the governing failure mechanism. A similar level of precision was achieved using only analytical expressions when properly calibrated. Therefore, the CSCT expressions can be used at different stages of design and assessment of existing structures according to the Level of Approximation required.

Related References:

1. Lantsoght, E. O. L., van der Veen, C., and Walraven, J. C. “Shear in one-way slabs under concentrated load close to support,” ACI Structural Journal, V. 110, No. 2, 2013, pp. 275–84.

2. Lantsoght, E. O. L., van der Veen, C., Walraven, J. C., et al. “Database of wide concrete members failing in shear,” Magazine of Concrete Research, V. 67, No. 1, 2015, pp. 33–52.

3. Natário, F., Fernández Ruiz, M., and Muttoni, A. “Shear strength of RC slabs under concentrated loads near clamped linear supports,” Engineering Structures, V. 76, No. September, 2014, pp. 10–23.

4. de Sousa, A. M. D., Lantsoght, E. O. L., Setiawan, A., et al. “Transition from one-way to two-way shear by coupling LEFEA and the CSCT models.” Proceedings of the fib Symposium 2021, Concrete Structures: New Trends for Eco-Efficiency and Performance. Lisbon, Portugal, 2021.

5. Halvonik, J., Vidaković, A., and Vida, R. “Shear Capacity of Clamped Deck Slabs Subjected to a Concentrated Load,” Journal of Bridge Engineering, V. 25, No. 7, 2020, p. 04020037.

6. FD P 18-717. “Eurocode 2 - Calcul des structures en béton - Guide d’application des normes NF EN 1992,” 2013.

7. Bui, T. T., Abouri, S., Limam, A., et al. “Experimental investigation of shear strength of full-scale concrete slabs subjected to concentrated loads in nuclear buildings,” Engineering Structures, V. 131, 2017, pp. 405–20.

8. Reißen, K. “Zum Querkrafttragverhalten von einachsig gespannten Stahlbe- tonplatten ohne Querkraftbewehrung unter Einzellasten.” Doctor of Engineering, PhD Thesis (Doctor of Engineering), Faculty of Civil Engineering, RWTH Aachen University, Aachen, Germany, 2016.

9. de Sousa, A. M. D., Lantsoght, E. O. L., Yang, Y., et al. “Extended CSDT model for shear capacity assessments of bridge deck slabs,” Engineering Structures, V. 234, 2021, p. 111897.

10. Sousa, A. M. D., and el Debs, M. K. “Shear strength analysis of slabs without transverse reinforcement under concentrated loads according to ABNT NBR 6118:2014,” IBRACON Structures and Materials Journal, V. 12, No. 3, 2019, pp. 658–93.

11. Natário, F. “Static and Fatigue Shear Strength of Reinforced Concrete Slabs Under Concentrated Loads Near Linear Support.” PhD Thesis (Docteur ès Sciences), École Polytechnique Fédérale de Lausanne, 2015.

12. Fédération Internationale du Béton (fib). “fib Model Code for Concrete Structures 2010,” v. vol. 1–2, Lausanne, Switzerland, Ernst & Sohn - fédération internationale du béton, Bulletin 65, 2012.

13. Rombach, G., and Henze, L. “Querkrafttragfähigkeit von Stahlbetonplatten ohne Querkraftbewehrung unter konzentrierten Einzellasten,” Beton- und Stahlbetonbau, V. 112, No. 9, 2017, pp. 568–78.

14. Vida, R., and Halvonik, J. “Experimentálne overovanie šmykovej odolnosti mostovkových dosiek (Experimental verification of shear resistance of bridge deck slabs),” Inžinierske stavby/Inženýrské stavby, No. 4, 2018, pp. 2–6.

15. Lantsoght, E. O. L., van der Veen, C., Walraven, J. C., et al. “Transition from one-way to two-way shear in slabs under concentrated loads,” Magazine of Concrete Research, V. 67, No. 17, 2015, pp. 909–22.

16. Fernández Ruiz, M., Vaz Rodrigues, R., and Muttoni, A. “Dimensionnement et vérification des dalles de roulement des ponts routiers,” Rapport: Projet de recherche AGB 2002/028 sur demande du Groupe de travail Recherche en matière de ponts (AGB), 2009.

17. Henze, L., Rombach, G. A., and Harter, M. “New approach for shear design of reinforced concrete slabs under concentrated loads based on tests and statistical analysis,” Engineering Structures, V. 219, No. May, 2020, p. 110795.

18. Vaz Rodrigues, R., Fernández Ruiz, M., and Muttoni, A. “Shear strength of R/C bridge cantilever slabs,” Engineering Structures, V. 30, 2008, pp. 3024–33.

19. Goldbeck, A. T. “The Influence of Total Width of the Effective Width of Reinforced-Concrete Slabs Subjected to Central Concentrated Loading,” ACI Journal Proceedings, V. 13, No. 2, 1917, pp. 78–88.

20. Lantsoght, E. O. L., de Boer, A., and van der Veen, C. “Distribution of peak shear stress in finite element models of reinforced concrete slabs,” Engineering Structures, V. 148, 2017, pp. 571–83.

21. Goldbeck, A. T., and Smith, E. B. “Tests of Large Reinforced Concrete Slabs,” ACI Journal Proceedings, V. 12, No. 2, 1916, pp. 324–33.

22. Lantsoght, E. O. L., van der Veen, C., de Boer, A., et al. “Influence of width on shear capacity of reinforced concrete members,” ACI Structural Journal, V. 111, No. 6, 2014, pp. 1441–9.

23. Reißen, K., Classen, M., and Hegger, J. “Shear in reinforced concrete slabs-Experimental investigations in the effective shear width of one-way slabs under concentrated loads and with different degrees of rotational restraint,” Structural Concrete, V. 19, No. 1, 2018, pp. 36–48.

24. Lantsoght, E. O. L., van der Veen, C., Walraven, J. C., et al. “Peak shear stress distribution in finite element models of concrete slabs.” In: Zingoni, A., ed. Research and Applications in Structural Engineering, Mechanics and Computation. London, UK, CRC Press, Taylor & Francis Group, 2013. pp. 475–80.

25. Muttoni, A. “Punching Shear Strength of Reinforced Concrete Slabs without Transverse Reinforcement,” ACI Structural Journal, V. 105, No. 4, 2008, pp. 440–50.

26. Sagaseta, J., Muttoni, A., Fernández Ruiz, M., et al. “Non-axis-symmetrical punching shear around internal columns of RC slabs without transverse reinforcement,” Magazine of Concrete Research, V. 63, No. 6, 2011, pp. 441–57.

27. Muttoni, A., and Fernandez Ruiz, M. “Shear in slabs and beams: should they be treated in the same way?” FIB Bulletin 57: shear and punching shear in RC and FRC elements. 2010. pp. 105–28.

28. Muttoni, A., and Fernandez Ruiz, M. “Shear Strength of Members without Transverse Reinforcement as Function of Critical Shear Crack Width,” ACI Structural Journal, V. 105, No. 2, 2008, pp. 163–72.

29. Muttoni, A., and Schwartz, J. “Behavior of Beams and Punching in Slabs without Shear Reinforcement,” IABSE Colloquium, V. 62, No. January 1991, 1991, pp. 703–8.

30. Kani, G. N. J. “The Riddle of Shear Failure and its Solution,” ACI Journal Proceedings, V. 61, No. 4, 1964, pp. 441–68.

31. Walraven, J. C. “Fundamental Analysis of Aggregate Interlock,” Journal of the Structural Division, ASCE, V. 107, No. 11, 1981, pp. 2245–2270.

32. Dulacska, H. “Dowel Action of Reinforcement Crossing Cracks in Concrete,” ACI Journal Proceedings, V. 69, No. 12, 1972, pp. 754–7.

33. Taylor, H. P. “Investigation of the dowel shear forces carried by the tensile steel in reinforced concrete beams,” Cement and Concrete Association, 1969.

34. Vecchio, F. J., and Collins, M. P. “The Modified Compression-Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, 1986, pp. 219–31.

35. Belletti, B., Scolari, M., Muttoni, A., et al. “Shear strength evaluation of RC bridge deck slabs according to CSCT with multi – layered shell elements and PARC_CL Crack Model.” IABSE Conference Geneva 2015. Geneva, Switzerland, 2015. pp. 1158–65.

36. Sagaseta, J., Tassinari, L., Fernández Ruiz, M., et al. “Punching of flat slabs supported on rectangular columns,” Engineering Structures, V. 77, 2014, pp. 17–33.

37. Setiawan, A., Vollum, R. L., Macorini, L., et al. “Punching of RC slabs without transverse reinforcement supported on elongated columns,” Structures, V. 27, 2020, pp. 2048–68.

38. Cavagnis, F., Fernández Ruiz, M., and Muttoni, A. “A mechanical model for failures in shear of members without transverse reinforcement based on development of a critical shear crack,” Engineering Structures, V. 157, 2018, pp. 300–15.

39. Belletti, B., Damoni, C., Hendriks, M. A. N., et al. “Analytical and numerical evaluation of the design shear resistance of reinforced concrete slabs,” Structural Concrete, V. 15, No. 3, 2014, pp. 317–30.

40. Dassault Systems Simulia Corp. “Abaqus Analysis user’s manual 6.14,” Providence, Rhode Island (USA), Dassault Systems Simulia Corp., 2014.

41. Damasceno, L. S. R. “Experimental analysis of one-way reinforced concrete flat slabs in punching shear with rectangular columns (in Portuguese: Análise experimental de lajes lisas unidirecionais de concreto armado com pilares retangulares ao puncionamento).” Masters’ thesis, Departamento de Engenharia Civil, Universidade Federal do Pará, 2007.

42. Ferreira, M. de P. “Experimental analysis of one-way reinforced concrete flat slabs in axis or non-axissymmetric punching shear (in Portuguese: Análise experimental de lajes lisas unidirecionais de concreto armado ao puncionamento simétrico ou assimétrico).” Masters’ thesis, Universidade Federal do Pará, 2006.

43. Regan, P. E., and Rezai-Jorabi, H. “Shear Resistance of One-Way Slabs Under Concentrated Loads.,” ACI Structural Journal, V. 85, No. 2, 1988, pp. 150–7.

44. Lantsoght, E. O. L., de Boer, A., van der Veen, C., et al. “Effective shear width of concrete slab bridges,” Proceedings of the Institution of Civil Engineers - Bridge Engineering, V. 168, No. 4, 2015, pp. 287–98.

45. ACI Committee 318. “Building Code Requirements for Structural Concrete (ACI 318-19),” 2019, p. 988.