Compressive Cyclic Response of Steel Fiber-Reinforced Lightweight Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Compressive Cyclic Response of Steel Fiber-Reinforced Lightweight Concrete

Author(s): Hooshang Dabbagh, Khandaker M. Anwar Hossain, and Kasra Amoorezaei

Publication: Materials Journal

Volume: 120

Issue: 3

Appears on pages(s): 19-30

Keywords: compressive behavior; cyclic loading; lightweight concrete; steel fiber; stress-strain model

DOI: 10.14359/51738706

Date: 5/1/2023

Abstract:
The current study examines the effect of steel fiber content on the uniaxial compressive response of lightweight concrete to propose a stress-strain model in cyclic loading. For this purpose, 150 x 300 mm cylindrical specimens containing different volume ratios of steel fiber (0, 0.5, 1, and 1.5%) were tested to plot the cyclic curves of steel fiber-reinforced lightweight aggregate concrete (SFRLWAC). The best combination of two types of steel fibers was used in this research: straight hooked-end and crimped fibers with aspect ratios of 50 and 28.5, respectively. Key points on cyclic curves were examined, and the compressive behavior of lightweight concrete was investigated. The results show that the integration of steel fibers reduces the plastic strain and stiffness degradation of the reloading paths. Furthermore, a rise in steel fiber volume fraction is associated with increased common-point coordinates. A stress-strain relationship was proposed to define the compressive cyclic behavior of SFRLWAC. The model was compared with the experimental findings to confirm its validity. The proposed model shows satisfactory agreement with the experimental results.

Related References:

1. Popovics, S., “A Numerical Approach to the Complete Stress-Strain Curve of Concrete,” Cement and Concrete Research, V. 3, No. 5, Sept. 1973, pp. 583-599. doi: 10.1016/0008-8846(73)90096-3

2. Kumar, P., “A Compact Analytical Material Model for Unconfined Concrete under Uni-Axial Compression,” Materials and Structures, V. 37, No. 9, Nov. 2004, pp. 585-590. doi: 10.1007/BF02483287

3. Yankelevsky, D. Z., and Reinhardt, H. W., “Model for Cyclic Compressive Behavior of Concrete,” Journal of Structural Engineering, ASCE, V. 113, No. 2, Feb. 1987, pp. 228-240. doi: 10.1061/(ASCE)0733-9445(1987)113:2(228)

4. Sima, J. F.; Roca, P.; and Molins, C., “Cyclic Constitutive Model for Concrete,” Engineering Structures, V. 30, No. 3, Mar. 2008, pp. 695-706. doi: 10.1016/j.engstruct.2007.05.005

5. Sinha, B. P.; Gerstle, K. H.; and Tulin, L. G., “Stress-Strain Relations for Concrete under Cyclic Loading,” ACI Journal Proceedings, V. 61, No. 2, Feb. 1964, pp. 195-212.

6. Karsan, I. D., and Jirsa, J. O., “Behavior of Concrete under Compressive Loadings,” Journal of the Structural Division, ASCE, V. 95, No. 12, Dec. 1969, pp. 2543-2564. doi: 10.1061/JSDEAG.0002424

7. Bahn, B. Y., and Hsu, C.-T. T., “Stress-Strain Behavior of Concrete under Cyclic Loading,” ACI Materials Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 178-193.

8. Thienel, K.-C.; Haller, T.; and Beuntner, N., “Lightweight Concrete—From Basics to Innovations,” Materials (Basel), V. 13, No. 5, Mar. 2020, Article No. 1120. doi: 10.3390/ma13051120

9. Mo, K. H.; Alengaram, U. J.; and Jumaat, M. Z., “Bond Properties of Lightweight Concrete – A Review,” Construction and Building Materials, V. 112, June 2016, pp. 478-496. doi: 10.1016/j.conbuildmat.2016.02.125

10. Hwang, C.-L., and Hung, M.-F., “Durability Design and Performance of Self-Consolidating Lightweight Concrete,” Construction and Building Materials, V. 19, No. 8, Oct. 2005, pp. 619-626. doi: 10.1016/j.conbuildmat.2005.01.003

11. Bilodeau, A.; Kodur, V. K. R.; and Hoff, G. C., “Optimization of the Type and Amount of Polypropylene Fibres for Preventing the Spalling of Lightweight Concrete Subjected to Hydrocarbon Fire,” Cement and Concrete Composites, V. 26, No. 2, Feb. 2004, pp. 163-174. doi: 10.1016/S0958-9465(03)00085-4

12. Rossignolo, J. A.; Agnesini, M. V. C.; and Morais, J. A., “Properties of High-Performance LWAC for Precast Structures with Brazilian Lightweight Aggregates,” Cement and Concrete Composites, V. 25, No. 1, Jan. 2003, pp. 77-82. doi: 10.1016/S0958-9465(01)00046-4

13. Haque, M. N.; Al-Khaiat, H.; and Kayali, O., “Strength and Durability of Lightweight Concrete,” Cement and Concrete Composites, V. 26, No. 4, May 2004, pp. 307-314. doi: 10.1016/S0958-9465(02)00141-5

14. Zhang, M.-H., and Gjørv, O. E., “Mechanical Properties of High-Strength Lightweight Concrete,” ACI Materials Journal, V. 88, No. 3, May-June 1991, pp. 240-247.

15. Chang, T.-P., and Shieh, M.-M., “Fracture Properties of Lightweight Concrete,” Cement and Concrete Research, V. 26, No. 2, Feb. 1996, pp. 181-188. doi: 10.1016/0008-8846(95)00198-0

16. Wang, H.; Wei, M.; Wu, Y.; Huang, J.; Chen, H.; and Cheng, B., “Mechanical Behavior of Steel Fiber-Reinforced Lightweight Concrete Exposed to High Temperatures,” Applied Sciences (Basel), V. 11, No. 1, Jan. 2021, Article No. 116. doi: 10.3390/app11010116

17. Zhao, M.; Zhao, M.; Chen, M.; Li, J.; and Law, D., “An Experimental Study on Strength and Toughness of Steel Fiber Reinforced Expanded-Shale Lightweight Concrete,” Construction and Building Materials, V. 183, Sept. 2018, pp. 493-501. doi: 10.1016/j.conbuildmat.2018.06.178

18. Ye, Y.; Liu, J.; Zhang, Z.; Wang, Z.; and Peng, Q., “Experimental Study of High-Strength Steel Fiber Lightweight Aggregate Concrete on Mechanical Properties and Toughness Index,” Advances in Materials Science and Engineering, V. 2020, 2020, Article No. 5915034. doi: 10.1155/2020/5915034

19. Hassanpour, M.; Shafigh, P.; and Mahmud, H. B., “Lightweight Aggregate Concrete Fiber Reinforcement – A Review,” Construction and Building Materials, V. 37, Dec. 2012, pp. 452-461. doi: 10.1016/j.conbuildmat.2012.07.071

20. Wu, Z.; Shi, C.; He, W.; and Wu, L., “Effects of Steel Fiber Content and Shape on Mechanical Properties of Ultra High Performance Concrete,” Construction and Building Materials, V. 103, Jan. 2016, pp. 8-14. doi: 10.1016/j.conbuildmat.2015.11.028

21. Suraneni, P.; Bran Anleu, P. C.; and Flatt, R. J., “Factors Affecting the Strength of Structural Lightweight Aggregate Concrete with and without Fibers in the 1,200–1,600 kg/m3 Density Range,” Materials and Structures, V. 49, No. 1-2, Jan. 2016, pp. 677-688. doi: 10.1617/s11527-015-0529-2

22. Bentur, A., and Mindess, S., Fibre Reinforced Cementitious Composites, CRC Press, Boca Raton, FL, 2006.

23. Akbarpour, S.; Dabbagh, H.; and Tavakoli, H. R., “The Effects of Steel Fiber and Nano-SiO2 on the Cyclic Flexural Behavior of Reinforced LWAC Beams,” KSCE Journal of Civil Engineering, V. 22, No. 10, Oct. 2018, pp. 3919-3930. doi: 10.1007/s12205-017-0920-3

24. Li, C.; Zhao, M.; Zhang, X.; Li, J.; Li, X.; and Zhao, M., “Effect of Steel Fiber Content on Shear Behavior of Reinforced Expanded-Shale Lightweight Concrete Beams with Stirrups,” Materials (Basel), V. 14, No. 5, Mar. 2021, Article No. 1107. doi: 10.3390/ma14051107

25. Spinella, N.; Colajanni, P.; and La Mendola, L., “Nonlinear Analysis of Beams Reinforced in Shear with Stirrups and Steel Fibers,” ACI Structural Journal, V. 109, No. 1, Jan.-Feb. 2012, pp. 53-64.

26. Susetyo, J.; Gauvreau, P.; and Vecchio, F. J., “Effectiveness of Steel Fiber as Minimum Shear Reinforcement,” ACI Structural Journal, V. 108, No. 4, July-Aug. 2011, pp. 488-496.

27. Campione, G., and La Mendola, L., “Stress-Strain Behavior in Compression of Lightweight Fiber Reinforced Concrete under Monotonic and Cyclic Loads,” WIT Transactions on the Built Environment, V. 57, Aug. 2001, pp. 387-396.

28. Campione, G., and La Mendola, L., “Behavior in Compression of Lightweight Fiber Reinforced Concrete Confined with Transverse Steel Reinforcement,” Cement and Concrete Composites, V. 26, No. 6, Aug. 2004, pp. 645-656. doi: 10.1016/S0958-9465(03)00047-7

29. Liu, X.; Wu, T.; and Liu, Y., “Stress-Strain Relationship for Plain and Fibre-Reinforced Lightweight Aggregate Concrete,” Construction and Building Materials, V. 225, Nov. 2019, pp. 256-272. doi: 10.1016/j.conbuildmat.2019.07.135

30. Dabbagh, H.; Amoorezaei, K.; Akbarpour, S.; and Babamuradi, K., “Compressive Toughness of Lightweight Aggregate Concrete Containing Different Types of Steel Fiber under Monotonic Loading,” AUT Journal of Civil Engineering, V. 1, No. 1, May 2017, pp. 15-22.

31. Dabbagh, H., and Amoorezaei, K., “Stress-Strain Relationship for Steel Fiber-Reinforced Lightweight Aggregate Concrete under Uniaxial Compression,” Journal of Stress Analysis, V. 4, No. 1, 2019, pp. 43-52.

32. Campione, G.; Miraglia, N.; and Papia, M., “Mechanical Properties of Steel Fibre Reinforced Lightweight Concrete with Pumice Stone or Expanded Clay Aggregates,” Materials and Structures, V. 34, No. 4, May 2001, pp. 201-210. doi: 10.1007/BF02480589

33. ASTM C330/C330M-14, “Standard Specification for Lightweight Aggregates for Structural Concrete,” ASTM International, West Conshohocken, PA, 2014, 4 pp.

34. Amoorezaei, K., “Behavior of Steel Fiber-Reinforced Lightweight Concrete under Compressive Cyclic Loading,” MSc thesis, University of Kurdistan, Sanandaj, Kurdistan, Iran, 2016. (in Persian)

35. ACI Committee 211, “Standard Practice for Selecting Proportions for Structural Lightweight Concrete (ACI 211.2-98) (Reapproved 2004),” American Concrete Institute, Farmington Hills, MI, 1998, 20 pp.

36. ASTM C469/C469M-10, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2010, 5 pp.

37. ASTM C39/C39M-12, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2012, 7 pp.

38. Shah, S. P., and Winter, G., “Inelastic Behavior and Fracture of Concrete,” ACI Journal Proceedings, V. 63, No. 9, Sept. 1966, pp. 925-930.

39. Sturman, G. M.; Shah, S. P.; and Winter, G., “Microcracking and Inelastic Behavior of Concrete,” Flexural Mechanics of Reinforced Concrete, SP-12, American Concrete Institute, Farmington Hills, MI, 1965, pp. 473-499.

40. Sinaie, S.; Heidarpour, A.; Zhao, X. L.; and Sanjayan, J. G., “Effect of Size on the Response of Cylindrical Concrete Samples under Cyclic Loading,” Construction and Building Materials, V. 84, June 2015, pp. 399-408. doi: 10.1016/j.conbuildmat.2015.03.076

41. Hsu, L. S., and Hsu, C.-T. T., “Stress-Strain Behavior of Steel-Fiber High-Strength Concrete under Compression,” ACI Structural Journal, V. 91, No. 4, July-Aug. 1994, pp. 448-457.


ALSO AVAILABLE IN:

Electronic Materials Journal