Title: ASTM C94/C94M-21b, "Standard Specification for Ready-Mixed Concrete."

Author(s): ASTM Subcommittee C09.40 on Ready-Mixed Concrete

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C0094_C0094M-21B

Date: 10/1/2021

Abstract:
This specification covers ready-mixed concrete manufactured and delivered to a purchaser in freshly mixed and unhardened state as hereinafter specified. Requirements for quality of concrete shall be either as hereinafter specified or as specified by the purchase. In any case where the requirements of the purchaser differ from these in this specification, the purchaser's specification shall govern. In the absence of designated applicable materials specifications, materials specifications specified shall be used for cementitious materials, hydraulic cement, supplementary cementitious materials, cementitious concrete mixtures, aggregates, air-entraining admixtures, and chemical admixtures. Except as otherwise specifically permitted, cement, aggregate, and admixtures shall be measured by mass. Mixers will be stationary mixers or truck mixers. Agitators will be truck mixers or truck agitators. Test methods for compression, air content, slump, temperature shall be performed. For s strength test, at least two standard test specimens shall be made.




  

Edit Module Settings to define Page Content Reviewer