ASTM A775/A775M-19, "Standard Specification for Epoxy-Coated Steel Reinforcing Bars."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM A775/A775M-19, "Standard Specification for Epoxy-Coated Steel Reinforcing Bars."

Author(s): ASTM Subcommittee A01.05 on Steel Reinforcement

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/A0775_A0775M-19

Date: 6/1/2019

Abstract:
This specification covers deformed and plain steel reinforcing bars with protective epoxy coating applied by the electrostatic spray method. The surface of the steel reinforcing bars to be coated shall be cleaned by abrasive blast cleaning to near-white metal. The number and frequency of tests for coating thickness, continuity, flexibility and adhesion are specified. If the specimen for coating thickness or flexibility fails to meet the specified requirements, two retests on random samples shall be conducted for each failed test.