Title: Significance of the Fineness of Harvested Fly Ash and Ground Glass Pozzolans
Author(s): Mahipal Kasaniya
Publication: Web Session
Volume:
Issue:
Appears on pages(s):
Keywords:
DOI:
Date: 3/28/2022
Abstract: The purpose of this session is to offer authors/speakers an open forum for presentation of recent technical information that does not fit into other sessions scheduled for this convention.