Effect of Flexural Reinforcement Ratio, Effective Depth and Slenderness Ratio on Punching Strength or Spread Footings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Flexural Reinforcement Ratio, Effective Depth and Slenderness Ratio on Punching Strength or Spread Footings

Author(s): Neil M. Hawkins and Carlos E. Ospina

Publication: Symposium Paper

Volume: 353

Issue:

Appears on pages(s): 50-72

Keywords: Spread Footings; Footings; Foundations; Punching Shear; Shear Design; Size Effect

DOI: 10.14359/51737111

Date: 7/1/2022

Abstract:

The 2019 Edition of ACI 318 introduced several key changes to the one-way and two-way shear design of slabs. Chapter 22 introduced a size effect for the one-way and two-way shear strength of concrete for slabs either without or with shear reinforcement. ACI 318-19 also introduced a revised version of the Vc equation for one-way shear that included the effect of the member flexural reinforcement ratio. Chapter 8 of ACI 318-19 also introduced new minimum flexural reinforcement requirements to prevent premature punching failure of lightly-reinforced above grade two-way slabs and to promote instead a flexure-driven type of response. In ACI 318-19, recognition of the size effect is required for above grade slabs only and not for shallow footings or foundation mats. The Code is silent on whether the new Chapter 8 minimum flexural reinforcement requirements for slabs apply to spread footings.

This paper examines the reasons for the differences in size effect requirements between slabs and footings. It also evaluates the applicability and the impact that the new Vc equation for one-way shear has on the shear strength of isolated or continuous footings and whether the new flexural reinforcement requirements of Chapter 8 can be extended to spread footings. It also suggests a design recommendation to acknowledge the beneficial effect that compact footing dimensions can have on punching strength.

Related References:

1. ACI Committee 318-19, 2019, “Building Code Requirements for Structural Concrete and Commentary ACI 318-19,” American Concrete Institute, Farmington Hill, MI.

2. ACI-ASCE Committee 326, 1962, “Shear and Diagonal Tension-Part 3, Slabs and Footings” ACI Journal, Proceedings V.59, No.3, Mar. pp. 351-396.

3. Ahmed, F. R., Hamad, K. K., and Rashied, Z. N., 2017, “Prediction of Punching Strength of Reinforced Concrete Footings by Finite Element Method,” American Journal of Civil Engineering and Architecture, Vol. 5, No. 1, p. 8-16.

4. Alexander, S.D.B. and Hawkins, N.M., 2005, “A Design Perspective on Punching Shear,” Punching Shear in Reinforced Concrete Slabs, ACI SP-232, Polak, M. Ed., American Concrete Institute, Farmington Hills, MI, May, p.97-108.

5. Birkle, G., 2004, “Punching of Flat Slabs: The Influence of Slab Thickness and Stud Layout”, Ph. D. Thesis, University of Calgary. Calgary. Alberta, 152 p.

6. Canadian Standards Association, 2014, “Design of Concrete Structures CSA A23.3-14, Mississauga, Ontario.

7. Dam, T. X., Wight, J.K., Parra-Montesinos, and DaCosta, A., 2017, “Punching Failure of Slab-Column Connections Reinforced with Headed Shear Studs” Joint ACI-fib International

Symposium on Punching Shear of Structural Concrete Slabs, ACI SP-315/fib Bull. 81, Ospina, C.E., Mitchell, D., Muttoni, A., Eds., American Concrete Institute, Farmington Hills, MI, May, p.117-142.

8. Dönmez, A., and Bazant, Z.P., 2016, “Size Effect on Punching Strength of Reinforced concrete Slabs Without and With Shear Reinforcement,” Report N. 15-12/936s, Civil and Environmental Engineering, Northwestern University, Evanston, IL, p.23.

9. Guandalini, S., Burdet, O. and Muttoni, A., 2009, “Punching Tests of Slabs with Low Reinforcement Ratios”, ACI Structural Journal, Vol. 106, No. 1, Jan.-Feb., pp. 87-95.

10. Hawkins, N.M. and Ospina, C, E., 2017, “Effect of Slab Flexural Reinforcement and Depth on Punching Strength” Joint ACI-fib International Symposium on Punching Shear of Structural Concrete Slabs, ACI SP-315/fib Bull. 81, Ospina, C.E., Mitchell, D., Muttoni, A., Eds., American Concrete Institute, Farmington Hills, MI, May, p.117-142.

11. Hegger, J., Sherif, A.G., and Ricker, M., 2006, “Experimental Investigations on Punching Behavior of Reinforced Concrete Footings,” ACI Structural Journal, July-August, pp. 604-613.

12. Hegger, J., Ricker, M., and Sherif, A. G., 2009, “Punching Strength of Reinforced Concrete Footings,” ACI Structural Journal, V. 106, No.5, pp. 706-716.

13. Kinnunen, S., Nylander, H., and Tolf, P., 1980, “Influence of Slab Thickness on the Strength of Concrete Slabs at Punching, Tests with Rectangular Slabs”, Bulletin 137, Division of Building Statics and Structural Engineering, Royal Institute of Technology, Stockholm.

14. Kuchma, D.A., Wei, S.W., Sanders, D.H., Belarbi, A. and Nowak, L., 2019, “Development of the One-way shear Design Provisions of ACI 318-19 for Reinforced Concrete,” ACI Structural Journal, July, pp. 285-295.

15. Li, K. K. L., 2000, “Influence of Size on Punching Strength of Concrete Slabs“, M. Eng. Thesis Department of Civil Engineering and Applied Mechanics, McGill University, Montreal, Quebec, 78p.

16. Moe, J., 1961 “Shearing Strength of Reinforced Concrete Slabs and Footings Under Concentrated Loads,” Development Department Bulletin D 47, Portland Cement Association, Skokie, IL, 135 pp.

17. Muttoni, A., 2008, “Punching Shear Strength of Reinforced Concrete Slabs without Shear Reinforcement,” ACI Structural Journal, Vol. 105, No. 4, July-August, pp. 440-450.

18. Nylander, H. and Sundquist, H.,1972, “Punching of Bridge Slabs with Untensioned Reinforcement on Columns,” Bulletin 104, Division of Building Statics and Structural Engineering, Royal Institute of Technology, Stockholm.

19. Ospina, C.E., Birkle, G., Widianto, Fernando, S.R., Fernando, S., Catlin, A.C. Pujol, S., Monical, J. and Genikomsou, K., 2011, “ACI 445/fib WG 2.2.3 Punching Shear Test Databank 1,” http://datacenterhub.org/deedsdv/pubications/view/436.

20. Ospina, C. E., Birkle, G., and Widianto, 2012, “Databank of Concentric Punching Shear Tests of Two-way Concrete Slabs without Shear Reinforcement at Interior Supports,” 2012 ASCE Structures Congress, Proceedings, pp. 1814-1832.

21. Ospina, C.E. and Hawkins, N.M., 2013, “Addressing Punching Failure,” ASCE Structure Magazine, Jan.

22. Peiris, C., and Ghali, A., 2012, “Flexural Reinforcement Essential for Punching Shear Resistance of Slabs,” SP 287-06 Recent Developments in Reinforced Concrete Slab Analysis, Design and Serviceability, American Concrete Institute, Farmington Hills, MI, May.

23. Regan, P.E., 1986, “Symmetric Punching Shear of Reinforced Concrete Slabs,” Magazine of Concrete Research, Vol. 30, No. 136, Sept. pp. 115-128.

24. Richart, F.E., 1948, “Reinforced Concrete Walls and Column Footings- Parts 1 and 2,” ACI Journal, Vol. 45 pp. 97-127 and 237-260.

25. Sherwood, E.G., Bentz, E.C., and Collins, M.P., 2007, “The Effect of Aggregate Size on the Beam-Shear Strength of Thick Slabs”, ACI Structural Journal, V.104, No.2, March, pp.180-190.

26. Siburg, C. and Hegger, J., 2014, “Experimental Investigations on the punching behavior of reinforced concrete footings with structural dimensions,” fib Structural Concrete, V. 15, No. 3, pp. 331-339.

27. Simões, J.T., Bujnak, J., Fernandez Ruiz M., and Muttoni, A., 2016, “Punching Shear Tests on Compact Footings with Uniform Soil Pressure,” Structural Concrete, No. 4, fib, Suisse, pp. 603-617.

28. Stein, T., Ghali, A., and Dilger, W., 2007 “Distinction Between Punching and Flexural Failure Modes of Flat Plates,” ACI Structural Journal, V. 104, No. 3, May-June, pp. 357-365.

29. Widianto, Bayrak, O. and Jirsa, J.O., 2009, “Two-way Shear Strength of Slab-Column Connections: Reexamination of ACI 318 Provisions,” ACI Structural Journal, V. 106, No. 2, March-April, pp. 160-170.