Title:
Experimental and Theoretical Investigation on the Adsorbed Layer Thickness of PCE Comb Polymers
Author(s):
Johann Plank, Johannes Stecher, Constantin Tiemeyer
Publication:
Symposium Paper
Volume:
354
Issue:
Appears on pages(s):
1-12
Keywords:
polycarboxylate; superplasticizer; adsorption; cement; steric hindrance; adsorbed conformation; molecular dynamics (MD) simulation; dynamic light scattering (DLS); nanoparticles
DOI:
10.14359/51736057
Date:
7/1/2022
Abstract:
The dosage-dependent development of the adsorbed layer thickness (ALT) of two polycondensate (BNS, AFS), four polycarboxylate (23MPEG6, 45MPEG6, 52IPEG2, 52IPEG6), and one phosphate comb polymer (45MPEG-P3) was investigated via dynamic light scattering technique using cationic polystyrene nanoparticles as substrate. It was found that polycondensates develop very thin adsorbed layers [0.3 - 0.6 nm (1.2 - 2.4 × 10-8 in.)] whereas PCEs produce layers of ~ 2.5 - 8 nm (9.8 - 31 × 10-8 in.). These values are larger than those reported previously from AFM and XPS measurements but correlate well with results from molecular dynamics simulations. For PCE molecules, the side chain length exercises the most significant effect on the adsorbed layer thickness while the grafting density has less impact. Furthermore, stronger anchor groups such as the phosphate copolymer produce more dense polymer layers and hence higher ALT values which explain their excellent dispersing effectiveness. Spread flow tests using cement paste revealed a relatively close relationship between paste fluidity and ALT.
Related References:
1. Derjaguin, B., and Landau, L., “The theory of stability of highly charged lyophobic sols and coalescence of highly charged particles in electrolyte solutions”, Acta Physicochim. URSS, V. 14, No. 633-52, 1941, pp. 58.
2. Verwey, E. J. W., Overbeek, J. T. G., Van Nes, K., “The Interaction of Sol Particles Having an Electric Double Layer”, Theory of the Stability of Lyophobic Colloids, Elsevier Publishing Company, 1948.
3. Ottewill, R. H., and Walker, T., “The influence of non-ionic surface active agents on the stability of polystyrene latex dispersions”, Kolloid-Zeitschrift und Zeitschrift für Polymere, V. 227, No. 1, 1968, pp. 108-116.
4. Yoshioka, K., Sakai, E., Daimon, M., and Kitahara, A., “Role of steric hindrance in the performance of superplasticizers for concrete”, J. Am. Ceram. Soc., V. 80, No. 10, 1997, pp. 2667-2671.
5. Sakai, E., Yamada, K., and Ohta, A., “Molecular Structure and Dispersion-Adsorption Mechanisms of Comb-Type Superplasticizers Used in Japan”, Journal of Advanced Concrete Technology, V. 1, 2003, pp. 16-25.
6. Birdi, K., “Handbook of surface and colloid chemistry”, CRC press, 2015.
7. Plank, J., Li, H., Ilg, M., Pickelmann, J., Eisenreich, W., Yao, Y., and Wang, Z., “A microstructural analysis of isoprenol ether-based polycarboxylates and the impact of structural motifs on the dispersing effectiveness”, Cement and Concrete Research, V. 84, 2016, pp. 20-29.
8. Plank, J., Schroefl, C., Gruber, M., Lesti, M., and Sieber, R., “Effectiveness of polycarboxylate superplasticizers in ultra-high strength concrete: the importance of PCE compatibility with silica fume”, Journal of Advanced Concrete Technology, V. 7, No. 1, 2009, pp. 5-12.
9. Kauppi, A., Andersson, K. A., and Bergstrom, L., “Probing the effect of superplasticizer adsorption on the surface forces using the colloidal probe AFM technique”, Cement and Concrete Research, V. 35, No. 1, 2005, pp. 133-140.
10. Flatt, R. J., Schober, I., Raphael, E., Plassard, C., and Lesniewska, E., “Conformation of Adsorbed Comb Copolymer Dispersants”, Langmuir, V. 25, No. 2, 2009, pp. 845-855.
11. Li-ying, W., Yan, X., Zhen-dong, J., Yong, X., Sheng, X., Xin-yu, G., and Xue-min, W., “A study of the adsorption property of dispersant of polycarboxylate onto pyraclostrobin particle surfaces by using FT-IR, XPS and SEM”, Spectroscopy and Spectral Analysis, V. 38, No. 11, 2018, pp. 3401-3406.
12. Zheng, T., Zheng, D., Qiu, X., Yang, D., Fan, L., and Zheng, J., “A novel branched claw-shape lignin-based polycarboxylate superplasticizer: Preparation, performance and mechanism”, Cement and Concrete Research, V. 119, 2019, pp. 89-101.
13. He, Y., Shu, X., Wang, X., Yang, Y., Liu, J., and Ran, Q., “Effects of polycarboxylates with different adsorption groups on the rheological properties of cement paste”, Journal of Dispersion Science and Technology, V. 41, No. 6, 2019, pp. 873-883.
14. Zhang, Y., Liu, H., Liu, J., and Tong, R., “Effect of Sodium Hexametaphosphate and Trisodium Phosphate on Dispersion of Polycarboxylate Superplasticizer”, Materials, V. 12, No. 24, 2019.
15. Wang, C., Meng, R., Wang, R., and Shen, Z., “Synthesis and mechanism study of gelatin grafted acetone formaldehyde sulphonates as oil-well cement dispersant”, RSC Advances, V. 7, No. 50, 2017, pp. 31779-31788.
16. Hirata, T., Ye, J., Branicio, P., Zheng, J., Lange, A., Plank, J., and Sullivan, M., “Adsorbed conformations of PCE superplasticizers in cement pore solution unraveled by molecular dynamics simulations”, Scientific Reports, V. 7, No. 1, 2017, pp. 1-10.
17. Yoshioka, K., Tazawa, E.-i., Kawai, K., and Enohata, T., “Adsorption characteristics of superplasticizers on cement component minerals”, Cement and Concrete Research, V. 32, No. 10, 2002, pp. 1507-1513.
18. Plank, J., and Hirsch, C., “Impact of zeta potential of early cement hydration phases on superplasticizer adsorption”, Cement and Concrete Research, V. 37, No. 4, 2007, pp. 537-542.
19. Kleshchanok, D., and Lang, P. R., “Steric repulsion by adsorbed polymer layers studied with total internal reflection microscopy”, Langmuir, V. 23, No. 8, 2007, pp. 4332-4339.
20. M. Collepardi, M. C., and Valente, M.,“Influence of Polymerization of Sulfonated Naphthalene Condensate and its Interaction with Cement”, SECOND CANMET/ACI International Conference on Superplasticizers in Concrete, Ottawa, Canada, 1981.
21. Plank, J., Dugonjic-Bilic, F., and Lummer, N. R., “Modification of the Molar Anionic Charge Density of Acetone-Formaldehyde-Sulfite Dispersant to Improve Adsorption Behavior and Effectiveness in the Presence of CaAMPS-co-NNDMA Cement Fluid Loss Polymer”, J. Appl. Polym. Sci., V. 111, No. 4, 2009, pp. 2018-2024.
22. Plank, J., Pöllmann, K., Zouaoui, N., Andres, P. R., and Schaefer, C., “Synthesis and performance of methacrylic ester based polycarboxylate superplasticizers possessing hydroxy terminated poly(ethylene glycol) side chains”, Cement and Concrete Research, V. 38, No. 10, 2008, pp. 1210-1216.
23. Yamamoto, M., Uno, T., Onda, Y., Tanaka, H., Yamashita, A., Hirata, T., and Hirano, N., “Copolymer for cement admixtures and its production process and use”, US Patent US 6727315 B2, 2004.
24. Stecher, J., and Plank, J., “Novel concrete superplasticizers based on phosphate esters”, Cement and Concrete Research, V. 119, 2019, pp. 36-43.
25. Kim, M. S., Kim, S. K., Lee, J. Y., Cho, S. H., Lee, K.-H., Kim, J., and Lee, S.-S., “Synthesis of polystyrene nanoparticles with monodisperse size distribution and positive surface charge using metal stearates”, Macromolecular Research, V. 16, No. 2, 2008, pp. 178-181.
26. European Norm DIN EN 1015-3: Methods of test for mortar for masonry – Part 3: Determination of consistence of fresh mortar (by flow table), DIN Deutsches Institut für Normung e. V..
27. Tiemeyer, C., Lange, A., and Plank, J., “Determination of the adsorbed layer thickness of functional anionic polymers utilizing chemically modified polystyrene nanoparticles”, Colloids and Surfaces A: Physicochemical and Engineering Aspects, V. 456, 2014, pp. 139-145.
28. Stecher, J., and Plank, J., “Adsorbed layer thickness of polycarboxylate and polyphosphate superplasticizers on polystyrene nanoparticles measured via dynamic light scattering”, J Colloid Interface Sci, V. 562, 2020, pp. 204-212.