Abstract:
The use of recycled concrete aggregate (RCA) from construction and demolition waste (CDW) in new concrete production is a promising solution to reduce the exploitation of non-renewable resources and landfill waste. Nowadays, only a small part of RCA is recycled due to severe regulatory restrictions in this field. Specifically, Italian Standards enable the use of solely coarse RCA and limit by 30% its substitution ratio to natural aggregate for structural concrete >C20/25 and ≤C30/37. In the present paper, concrete waste resulting from selective demolition was fully characterized and the high potential to develop green structural concrete using high RCA content was outlined. Substitution ratios of 30, 60, and 90vol% of natural aggregates were evaluated. Special attention was paid to the concrete mix design depending on the peculiar properties of RCA. Compressive strength tests at 3, 7, and 28 days of curing outlined the possibility to develop highly sustainable concrete of strength class C25/30. Thus, a viable and sustainable valorization of all particle size fractions was suggested, as well as the necessity of more permissive regulations based on the quality of the RCA used.
Related References:
1. Kisku, N.; Joshi, H.; Ansari, M.; Panda, S.K.; Nayak, S.; Dutta, S.C. A critical review and assessment for usage of recycled aggregate as sustainable construction material. Constr. Build. Mater. 2017, 131, 721–740.
2. ISPRA, I.S. per la P. e R.A. Produzione e gestione dei rifiuti speciali in Italia; 2018; Vol. 1;.
3. European Aggregates Association UEPG Annual Review 2019 - 2020. UEPG 2020, 31.
4. Tam, V.W.Y.; Soomro, M.; Evangelista, A.C.J. A review of recycled aggregate in concrete applications (2000–2017). Constr. Build. Mater. 2018, 172, 272–292, doi: 10.1016/j.conbuildmat.2018.03.240
5. Silva, R. V.; De Brito, J.; Dhir, R.K. Properties and composition of recycled aggregates from construction and demolition waste suitable for concrete production. Constr. Build. Mater. 2014, 65, 201–217, doi: 10.1016/j.conbuildmat.2014.04.117
6. Akhtar, A.; Sarmah, A.K. Construction and demolition waste generation and properties of recycled aggregate concrete: A global perspective. J. Clean. Prod. 2018, 186, 262–281, doi: 10.1016/J.JCLEPRO.2018.03.085
7. Barreto Santos, M.; de Brito, J.; Santos Silva, A.; Hasan Ahmed, H. Study of ASR in concrete with recycled aggregates: Influence of aggregate reactivity potential and cement type. Constr. Build. Mater. 2020, 265, 120743, doi: 10.1016/j.conbuildmat.2020.120743
8. Barreto Santos, M.; de Brito, J.; Santos Silva, A.; Hawreen, A. Effect of the source concrete with ASR degradation on the mechanical and physical properties of coarse recycled aggregate. Cem. Concr. Compos. 2020, 111.
9. He, P.; Zhang, B.; Lu, J.X.; Poon, C.S. ASR expansion of alkali-activated cement glass aggregate mortars. Constr. Build. Mater. 2020, 261, doi: 10.1016/j.conbuildmat.2020.119925
10. Trottier, C.; Zahedi, A.; Ziapour, R.; Sanchez, L.; Locati, F. Microscopic assessment of recycled concrete aggregate (RCA) mixtures affected by alkali-silica reaction (ASR). Constr. Build. Mater. 2021, 269, doi: 10.1016/j.conbuildmat.2020.121250
11. Sanchez-Cotte, E.H.; Fuentes, L.; Martinez-Arguelles, G.; Rondón Quintana, H.A.; Walubita, L.F.; Cantero-Durango, J.M. Influence of recycled concrete aggregates from different sources in hot mix asphalt design. Constr. Build. Mater. 2020, 259, doi: 10.1016/j.conbuildmat.2020.120427
12. Puente de Andrade, G.; de Castro Polisseni, G.; Pepe, M.; Toledo Filho, R.D. Design of structural concrete mixtures containing fine recycled concrete aggregate using packing model. Constr. Build. Mater. 2020, 252, doi: 10.1016/j.conbuildmat.2020.119091
13. Zhang, L.W.; Sojobi, A.O.; Kodur, V.K.R.; Liew, K.M. Effective utilization and recycling of mixed recycled aggregates for a greener environment. J. Clean. Prod. 2019, 236, doi: 10.1016/j.jclepro.2019.07.075
14. Khoury, E.; Ambrós, W.; Cazacliu, B.; Sampaio, C.H.; Remond, S. Heterogeneity of recycled concrete aggregates, an intrinsic variability. Constr. Build. Mater. 2018, 175, 705–713, doi: 10.1016/j.conbuildmat.2018.04.163
15. Nedeljković, M.; Visser, J.; Šavija, B.; Valcke, S.; Schlangen, E. Use of fine recycled concrete aggregates in concrete: A critical review. J. Build. Eng. 2021, 38, doi: 10.1016/j.jobe.2021.102196
16. Silva, R. V; De Brito, J.; Dhir, R.K. Performance of cementitious renderings and masonry mortars containing recycled aggregates from construction and demolition wastes. Constr. Build. Mater. 2016, 105, 400–415, doi: 10.1016/j.conbuildmat.2015.12.171
17. Jalilifar, H.; Sajedi, F. Micro-structural analysis of recycled concretes made with recycled coarse concrete aggregates. Constr. Build. Mater. 2021, 267, doi: 10.1016/j.conbuildmat.2020.121041
18. Etxeberria, M.; Vázquez, E.; Marí, A.; Barra, M. Influence of amount of recycled coarse aggregates and production process on properties of recycled aggregate concrete. Cem. Concr. Res. 2007, 37, 735–742, doi: 10.1016/j.cemconres.2007.02.002
19. Pedro, D.; de Brito, J.; Evangelista, L. Structural concrete with simultaneous incorporation of fine and coarse recycled concrete aggregates: Mechanical, durability and long-term properties. Constr. Build. Mater. 2017, 154, 294–309, doi: 10.1016/j.conbuildmat.2017.07.215