Title: Impact of Mixing Methods and Cement Dosage on Unconfined Compressive Strength of Cement-Stabilized Macadam

Author(s): Kaiyin Zhao, Lijun Zhao, Jinru Hou, Zhongxu Feng & Wenzhi Jiang

Publication: IJCSM

Volume: 16

Issue:

Appears on pages(s):

Keywords: cement stabilized macadam (CSM), unconfined compressive strength, vibratory mixing, cement dosage

DOI: 10.1186/s40069-022-00505-z

Date: 5/31/2022

Abstract: