Optimum Moisture Content of Substrate Prior to Applying Cementitious-Based Repair Materials (FAQ 28/364.XXT)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Optimum Moisture Content of Substrate Prior to Applying Cementitious-Based Repair Materials (FAQ 28/364.XXT)

Author(s): Jiang

Publication: Web Session

Volume: ws_S22_Jiang.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/28/2022

Abstract:
Achieving a lasting bond between repair materials and existing concrete is a critical requirement for durable concrete repair. Moisture conditioning of a prepared substrate has a direct effect on bond strength of repair material and the durability of repair. This presentation will discuss the factors that influence the formation of bond and the degree of adhesion, why the surface moisture condition of the substrate concrete is critical, and the test results associated with using a range of substrate moisture conditioning.