Upcycled Polypropylene and Polytrimethylene Terephthalate Carpet Waste in Reinforcing Cementitious Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Upcycled Polypropylene and Polytrimethylene Terephthalate Carpet Waste in Reinforcing Cementitious Composites

Author(s): Nghia P. Tran, Chamila Gunasekara, David W. Law, Shadi Houshyar, and Sujeeva Setunge

Publication: Materials Journal

Volume: 119

Issue: 4

Appears on pages(s): 125-138

Keywords: carpet waste; hybrid fiber combination; microstructure; nanoindentation; recycled fiber; X-ray micro-computed tomography (CT)

DOI: 10.14359/51734688

Date: 7/1/2022

Abstract:
In this study, carpet waste fibers—namely, polypropylene (PP) and polytrimethylene terephthalate (PTT) in the form of mono microfibers and hybrid combinations—were studied. The optimization of mono fiber parameters for fiber content (0.1, 0.3, and 0.5%) and length (6, 12, and 24 mm [0.236, 0.742, and 0.945 in.]) were conducted to achieve the optimum strength properties and minimize drying shrinkage. The microstructure, pore structure, and fiber-matrix interfacial properties of the optimized samples were characterized at 7, 28, and 90 days by means of scanning electron microscopy (SEM), X-ray micro-computed tomography (CT), and nanoindentation. The research data revealed that the inclusion of either the optimized mono PP fiber (υf = 0.5% and l = 12 mm [0.472 in.]) or PTT fiber (υf = 0.1% and l = 12 mm [0.472 in.]) improved the compressive strength of 4.3% and 16.1%, and the flexural strength by 11.5% and 9.2% at 28 days, respectively. Hybrid carpet fibers (0.4% PP + 0.1% PTT) provided a greater enhancement in compressive strength of 6.6%, and flexural strength by 13% at 28 days. Drying shrinkage mitigation of mortar over 120 days was recorded as 18.4, 22.3, and 25.8%, corresponding to the addition of 0.5% PP fibers, 0.1% PTT fibers, and hybrid PP/PTT carpet fibers. A pore-refining effect was also observed for mortars with 0.5% PP and hybrid PP/PTT carpet microfibers. The SEM images indicated that the trilobal cross-sectional shape of PTT carpet fibers had a stronger anchoring effect with cement hydrates than the rounded shape of PP carpet fibers. Nanoindentation identified the thickness of the fiber-matrix interfacial transition zone (ITZ) as approximately 15 μm (5.9 × 10–4 in.) for both mono PP and PTT fibers. Approximately 50% of the phases in the vicinity of the fiber-matrix interface comprised a porous structure at 7 days. However, the hydration of clinker over the 90-day period promoted the formation of calcium-silicate-hydrate (C-S-H) and portlandite to form a dense microstructure.

Related References:

1. Echeverria, C. A.; Handoko, W.; Pahlevani, F.; and Sahajwalla, V., “Cascading Use of Textile Waste for the Advancement of Fibre Reinforced Composites for Building Applications,” Journal of Cleaner Production, V. 208, Jan. 2019, pp. 1524-1536. doi: 10.1016/j.jclepro.2018.10.227

2. Debrabandere, P., “Swept under the Carpet: New Reports Reveal the Greenwash of the European Carpet Industry,” Zero Waste France, Paris, France, Feb. 2017.

3. European Commission, “Environment Policy & Governance: LIFE Projects 2012,” Publications Office of the European Union, Luxembourg City, Luxembourg, 2013, 157 pp.

4. Deutsche Umwelthilfe e.V. and Changing Markets, “Swept under the Carpet: The Big Waste Problem of the Carpet Industry in Germany,” Deutsche Umwelthilfe, Germany, 2017, 29 pp.

5. Eunomia Consulting, United Kingdom Without Incineration Network, and Changing Markets Foundation, “Smoke and Mirrors: Exposing the Reality of Carpet ‘Recycling’ in the UK,” Changing Markets Foundation, 2019, 9 pp.

6. Axion, “Zero Avoidable Waste in Flooring – Towards a Circular Economy,” Contract Flooring Association (CFA), Nottingham, UK, 2021, 50 pp.

7. Zeb-Kahn, A., “Carpet Recycling UK: Landfill Diversion of Carpet Waste Rises,” Carpet Recycling UK, Manchester, UK, 2019, https://carpetrecyclinguk.com/carpet-recycling-uk-landfill-diversion-of-carpet-waste-rises/. (last accessed May 25, 2022)

8. GAIA and Changing Markets, “Swept under the Carpet: Exposing the Greenwash of the U.S. Carpet Industry,” GAIA and Changing Markets, 2016, 25 pp.

9. United States Environmental Protection Agency, “Facts and Figures about Materials, Waste and Recycling,” EPA, Washington, DC, 2018, https://www.epa.gov/facts-and-figures-about-materials-waste-and-recycling/durable-goods-product-specific-data. (last accessed May 25, 2022)

10. NSW Environmental Protection Authority, “Disposal-Based Audit Commercial and Industrial Waste Stream in the Regulated Areas of New South Wales,” NSW EPA, Sydney, NSW, Australia, 2015, 474 pp.

11. Fashandi, H.; Pakravan, H. R.; and Latifi, M., “Application of Modified Carpet Waste Cuttings for Production of Eco-Efficient Lightweight Concrete,” Construction and Building Materials, V. 198, Feb. 2019, pp. 629-637. doi: 10.1016/j.conbuildmat.2018.11.163

12. Tran, N. P.; Gunasekara, C.; Law, D. W.; Houshyar, S.; Setunge, S.; and Cwirzen, A., “Comprehensive Review on Sustainable Fiber Reinforced Concrete Incorporating Recycled Textile Waste,” Journal of Sustainable Cement-Based Materials, V. 11, No. 1, 2022, pp. 28-42.

13. Awal, A. S. M. A., and Mohammadhosseini, H., “Green Concrete Production Incorporating Waste Carpet Fiber and Palm Oil Fuel Ash,” Journal of Cleaner Production, V. 137, Nov. 2016, pp. 157-166. doi: 10.1016/j.jclepro.2016.06.162

14. Ahmed, H. U.; Faraj, R. H.; Hilal, N.; Mohammed, A. A.; and Sherwani, A. F. H., “Use of Recycled Fibers in Concrete Composites: A Systematic Comprehensive Review,” Composites Part B: Engineering, V. 215, June 2021, Article No. 108769. doi: 10.1016/j.compositesb.2021.108769

15. Pakravan, H. R.; Jeddi, A. A. A.; Jamshidi, M.; Memarian, F.; and Saghafi, A. M., “Properties of Recycled Carpet Fiber Reinforced Concrete,” Use of Recycled Plastics in Eco-Efficient Concrete, F. Pacheco-Torgal, J. Khatib, F. Colangelo, and R. Tuladhar, eds., Woodhead Publishing, Sawston, UK, 2018, pp. 411-425.

16. Mohammadhosseini, H.; Tahir, M. M.; and Sayyed, M. I., “Strength and Transport Properties of Concrete Composites Incorporating Waste Carpet Fibres and Palm Oil Fuel Ash,” Journal of Building Engineering, V. 20, Nov. 2018, pp. 156-165. doi: 10.1016/j.jobe.2018.07.013

17. Mohammadhosseini, H.; Alyousef, R.; Abdul Shukor Lim, N. H.; Tahir, M. M.; Alabduljabbar, H.; and Mohamed, A. M., “Creep and Drying Shrinkage Performance of Concrete Composite Comprising Waste Polypropylene Carpet Fibres and Palm Oil Fuel Ash,” Journal of Building Engineering, V. 30, July 2020, Article No. 101250. doi: 10.1016/j.jobe.2020.101250

18. Mohammadhosseini, H.; Yatim, J. M.; Sam, A. R. M.; and Awal, A. S. M. A., “Durability Performance of Green Concrete Composites Containing Waste Carpet Fibers and Palm Oil Fuel Ash,” Journal of Cleaner Production, V. 144, Feb. 2017, pp. 448-458. doi: 10.1016/j.jclepro.2016.12.151

19. Mohammadhosseini, H.; Tahir, M. M.; Alaskar, A.; Alabduljabbar, H.; and Alyousef, R., “Enhancement of Strength and Transport Properties of a Novel Preplaced Aggregate Fiber Reinforced Concrete by Adding Waste Polypropylene Carpet Fibers,” Journal of Building Engineering, V. 27, Jan. 2020, Article No. 101003. doi: 10.1016/j.jobe.2019.101003

20. Zareei, S. A.; Ameri, F.; Bahrami, N.; Shoaei, P.; Musaeei, H. R.; and Nurian, F., “Green High Strength Concrete Containing Recycled Waste Ceramic Aggregates and Waste Carpet Fibers: Mechanical, Durability, and Microstructural Properties,” Journal of Building Engineering, V. 26, Nov. 2019, Article No. 100914. doi: 10.1016/j.jobe.2019.100914

21. Wu, X.; ; Zhou, J.; Kang, T.; Wang, F.; Ding, X.; and Wang, S., “Laboratory Investigation on the Shrinkage Cracking of Waste Fiber-Reinforced Recycled Aggregate Concrete,” Materials (Basel), V. 12, No. 8, Apr. 2019, Article No. 1196. doi: 10.3390/ma12081196

22. Wang, Y.; Zureick, A.-H.; Cho, B.-S.; and Scott, D. E., “Properties of Fibre Reinforced Concrete Using Recycled Fibres from Carpet Industrial Waste,” Journal of Materials Science, V. 29, No. 16, Aug. 1994, pp. 4191-4199. doi: 10.1007/BF00414198

23. Wang, Y., “Concrete Reinforcement with Recycled Fibers from Carpet Industrial Waste,” Journal of Materials in Civil Engineering, ASCE, V. 9, No. 3, Aug. 1997, pp. 103-104. doi: 10.1061/(ASCE)0899-1561(1997)9:3(103)

24. AS 3972-2010, “General Purpose and Blended Cements,” Standards Australia, Sydney, NSW, Australia, 2010, 19 pp.

25. ASTM C1437-15, “Standard Test Method for Flow of Hydraulic Cement Mortar,” ASTM International, West Conshohocken, PA, 2015, 2 pp.

26. ASTM C109/C109M-20b, “Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50 mm] Cube Specimens),” ASTM International, West Conshohocken, PA, 2020, 12 pp.

27. ASTM C348-20, “Standard Test Method for Flexural Strength of Hydraulic-Cement Mortars,” ASTM International, West Conshohocken, PA, 2020, 6 pp.

28. ASTM C157/C157M-17, “Standard Test Method for Length Change of Hardened Hydraulic-Cement Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2017, 8 pp.

29. Gautham, S., and Sasmal, S., “Recent Advances in Evaluation of Intrinsic Mechanical Properties of Cementitious Composites Using Nanoindentation Technique,” Construction and Building Materials, V. 223, Oct. 2019, pp. 883-897. doi: 10.1016/j.conbuildmat.2019.07.002

30. Hu, C., and Li, Z., “A Review on the Mechanical Properties of Cement-Based Materials Measured by Nanoindentation,” Construction and Building Materials, V. 90, Aug. 2015, pp. 80-90. doi: 10.1016/j.conbuildmat.2015.05.008

31. Qian, C.; Nie, Y.; and Cao, T., “Sulphate Attack‐Induced Damage and Micro‐Mechanical Properties of Concrete Characterized by Nano‐Indentation Coupled with X‐Ray Computed Tomography,” Structural Concrete, V. 17, No. 1, Mar. 2016, pp. 96-104. doi: 10.1002/suco.201400123

32. Xu, L.; Deng, F.; and Chi, Y., “Nano-Mechanical Behavior of the Interfacial Transition Zone between Steel-Polypropylene Fiber and Cement Paste,” Construction and Building Materials, V. 145, Aug. 2017, pp. 619-638. doi: 10.1016/j.conbuildmat.2017.04.035

33. Luo, Z.; Li, W.; Wang, K.; and Shah, S. P., “Research Progress in Advanced Nanomechanical Characterization of Cement-Based Materials,” Cement and Concrete Composites, V. 94, Nov. 2018, pp. 277-295. doi: 10.1016/j.cemconcomp.2018.09.016

34. Tran, N. P.; Gunasekara, C.; Law, D. W.; Houshyar, S.; Setunge, S.; and Cwirzen, A., “A Critical Review on Drying Shrinkage Mitigation Strategies in Cement-Based Materials,” Journal of Building Engineering, V. 38, June 2021, Article No. 102210. doi: 10.1016/j.jobe.2021.102210

35. Zhang, M., and Li, H., “Pore Structure and Chloride Permeability of Concrete Containing Nano-Particles for Pavement,” Construction and Building Materials, V. 25, No. 2, Feb. 2011, pp. 608-616. doi: 10.1016/j.conbuildmat.2010.07.032

36. Hernández-Cruz, D.; Hargis, C. W.; Dominowski, J.; Radler, M. J.; and Monteiro, P. J. M., “Fiber Reinforced Mortar Affected by Alkali-Silica Reaction: A Study by Synchrotron Microtomography,” Cement and Concrete Composites, V. 68, Apr. 2016, pp. 123-130. doi: 10.1016/j.cemconcomp.2016.02.003

37. Xue, G.; Yilmaz, E.; Song, W.; and Cao, S., “Analysis of Internal Structure Behavior of Fiber Reinforced Cement-Tailings Matrix Composites through X-ray Computed Tomography,” Composites Part B: Engineering, V. 175, Oct. 2019, Article No. 107091. doi: 10.1016/j.compositesb.2019.107091

38. Chinchillas-Chinchillas, M. J.; Orozco-Carmona, V. M.; Gaxiola, A.; Alvarado-Beltrán, C. G.; Pellegrini-Cervantes, M. J.; Baldenebro-López, F. J.; and Castro-Beltrán, A., “Evaluation of the Mechanical Properties, Durability and Drying Shrinkage of the Mortar Reinforced with Polyacrylonitrile Microfibers,” Construction and Building Materials, V. 210, June 2019, pp. 32-39. doi: 10.1016/j.conbuildmat.2019.03.178

39. Aly, T.; Sanjayan, J. G.; and Collins, F., “Effect of Polypropylene Fibers on Shrinkage and Cracking of Concretes,” Materials and Structures, V. 41, No. 10, Dec. 2008, pp. 1741-1753. doi: 10.1617/s11527-008-9361-2

40. Ramezanianpour, A. A.; Esmaeili, M.; Ghahari, S. A.; and Najafi, M. H., “Laboratory Study on the Effect of Polypropylene Fiber on Durability, and Physical and Mechanical Characteristic of Concrete for Application in Sleepers,” Construction and Building Materials, V. 44, July 2013, pp. 411-418. doi: 10.1016/j.conbuildmat.2013.02.076

41. Chinchillas-Chinchillas, M. J.; Pellegrini-Cervantes, M. J.; Castro-Beltrán, A.; Rodríguez-Rodríguez, M.; Orozco-Carmona, V. M.; and Peinado-Guevara, H. J., “Properties of Mortar with Recycled Aggregates, and Polyacrylonitrile Microfibers Synthesized by Electrospinning,” Materials (Basel), V. 12, No. 23, Dec. 2019, Article No. 3849. doi: 10.3390/ma12233849

42. Tran, N. P.; Gunasekara, C.; Law, D. W.; Houshyar, S.; and Setunge, S., “Microstructural Characterisation of Cementitious Composite Incorporating Polymeric Fibre: A Comprehensive Review,” Construction and Building Materials, V. 335, June 2022, Article No. 127497. doi: 10.3390/ma12233849

43. Pinto, J.; Peixoto, A.; Vieira, J.; Fernandes, L.; Morais, J.; Cunha, V. M. C. F.; and Varum, H., “Render Reinforced with Textile Threads,” Construction and Building Materials, V. 40, Mar. 2013, pp. 26-32. doi: 10.1016/j.conbuildmat.2012.09.099

44. Qin, Y.; Zhang, X.; and Chai, J., “Damage Performance and Compressive Behavior of Early-Age Green Concrete with Recycled Nylon Fiber Fabric under an Axial Load,” Construction and Building Materials, V. 209, June 2019, pp. 105-114. doi: 10.1016/j.conbuildmat.2019.03.094

45. Qin, Y.; Zhang, X.; Chai, J.; Xu, Z.; and Li, S., “Experimental Study of Compressive Behavior of Polypropylene-Fiber-Reinforced and Polypropylene-Fiber-Fabric-Reinforced Concrete,” Construction and Building Materials, V. 194, Jan. 2019, pp. 216-225. doi: 10.1016/j.conbuildmat.2018.11.042


ALSO AVAILABLE IN:

Electronic Materials Journal