Durability of a Bridge Column under Marine Environments

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Durability of a Bridge Column under Marine Environments

Author(s): Jun Wang and Yail J. Kim

Publication: Symposium Paper

Volume: 351

Issue:

Appears on pages(s): 70-82

Keywords: bridges; column; deterioration; durability; performance

DOI: 10.14359/51734675

Date: 4/1/2022

Abstract:
This paper presents a preliminary study on the durability of a bridge column under typical marine environments consisting of atmospheric, splash, and submerged conditions. To predict the migration of chlorides across the column, a simulation is conducted using a mathematical method, called cellular automata. Because chloride concentrations and the corrosion current density at the surface level of reinforcing steel can lead to the deterioration of a column over 100 years, they are of particular interest. The highest chloride concentrations are observed under the splash exposure, followed by the submerged and atmospheric conditions.




  