Title:
Analysis of an Existing Compressor Foundation with Excessive Local Vibration
Author(s):
O. S. Ali Ahmed and Damon G. Reigles
Publication:
Symposium Paper
Volume:
348
Issue:
Appears on pages(s):
47-69
Keywords:
Compressor foundation, soil-structure interaction, finite-element method, dynamic loading, machine foundation, stiffness, damping.
DOI:
10.14359/51732679
Date:
3/1/2021
Abstract:
This paper discusses the factors that affect the dynamic response of machine foundation systems, which include (1) the soil dynamic properties, (2) the geometric properties of the foundation, (3) mass of the machine and foundation, and (4) the amplitude and frequency of the applied dynamic loads. The primary objective in any
machine foundation design is to limit the foundation response below a specific amplitude threshold. A foundation response exceeding this limit may adversely affect the performance of the machine and damage the machine internals, resulting in costly repairs and lost revenue. Also, the excessive vibrations may result in structural degradation of the foundation, additional excitation stresses on the machine, and increase the compressor unbalance loading. This paper
presents dynamic analysis results of a four-cylinder compressor foundation originally designed without consideration
for soil-foundation interaction and suffering from excessive vibration. The foundation block supports a 4-cylinder
Dresser-Rand compressor, suction and discharge bottles, a crank, and a driving motor with a total weight of approximately 300 kip (1334 kN). A three-dimensional, finite element model representing the soil–foundation system was developed to determine the dynamic characteristics and assess the foundation response under applied dynamic loading from the compressor crank. Results showed that the response of the soil-foundation system is governed by the
response of the individual support piers (blocks) and not the global foundation response. This paper also provides a recommended modification to the foundation geometry to reduce the effect of the individual piers' local modes and enhance the foundation dynamic performance.
Related References:
1. ACI 351.3R-18 (2018). “Foundations for Dynamic Equipment,” Farmington Hill, MI.
2. ANSYS Inc. (2018). “Element Reference,” Release 19. Canonsburg, PA.
3. ASCE Manuals and Reports on Engineering Practice No. 136, (2018). “Concrete Foundations for Turbine Generators: Analysis, Design, and Construction,” American Society of Civil Engineering.
4. Kavvadas, M. and Gazetas, G. (1993). “Kinematic Seismic Response and Bending of Free-Head Piles in Layered Soil. Geotechnique,” 43, 2, pp. 207-222.
5. Kobori, T. (1962). “Dynamical Response of Rectangular Foundations on an Elastic – Space,” Proceedings, Japan National Symposium on Earthquake Engineering, Tokyo, Japan, pp.81-86.
6. Chae, Y.S. (1969). “Vibration of Non-Circular Foundations,” Journal of the Soil Mechanics and Foundations Division, American Society of Civil Engineering, Vol.95, No. SM6, pp.1411-1430.
7. Lysmer, J. and Kuhlemeyer, R.L. (1971). “Finite Dynamic Model for Infinite Media,” Journal of the Engineering Mechanics Divisions, ASCE, Vol.95, No.EM4, Proc. Paper 6719, Aug. 1969, p.859-877;
Closure, Vol.97, No. EM1, Proc. Paper 7862, Feb., pp.129-131.
8. Baxter, R.L., and Bernhard, D.L. (1967). “Vibration Tolerances for Industry,” ASME Paper 67-PEM-14, Plant Engineering and Maintenance Conference, Detroit, MI, Apr. 10-12.