On the Rate Sensitive Fracture Behavior of Strain-Hardening Cement-Based Composites (SHCC) Depending on Fiber Type and Matrix Composition

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: On the Rate Sensitive Fracture Behavior of Strain-Hardening Cement-Based Composites (SHCC) Depending on Fiber Type and Matrix Composition

Author(s): Iurie Curosu, Viktor Mechtcherine, Daniele Forni, Simone Hempel and Ezio Cadoni

Publication: Symposium Paper

Volume: 347

Issue:

Appears on pages(s): 1-20

Keywords: SHCC, fiber reinforcement, strain-hardening, PVA, UHMWPE, impact, split Hopkinson tension bar, fracture energy

DOI: 10.14359/51732655

Date: 3/1/2021

Abstract:

Synopsis: Strain-hardening cement-based composites (SHCC) represent a special type of fiber reinforced concretes, whose post-elastic tensile behavior is characterized by the formation of multiple, fine cracks under increasing loading up to failure localization. The high inelastic deformability in the strain-hardening phase together with the high damage tolerance and energy dissipation capacity make SHCC promising for applications involving dynamic loading scenarios, such as earthquake, impact or blast.

However, the main constitutive phases of SHCC, i.e. matrix, fibers and interphase between them, are highly rate sensitive. Depending on the SHCC composition, the increase in loading rates can negatively alter the balanced micromechanical interactions, leading to a pronounced reduction in strain capacity. Thus, there is need for a detailed investigation of the strain rate sensitivity of SHCC at different levels of observation for enabling a targeted material design with respect to high loading rates.

The crack opening behavior is an essential material parameter for SHCC, since it defines to a large extent the tensile properties of the composite. In the paper at hand, the rate effects on the crack opening and fracture behavior of SHCC are analyzed based on quasi-static and impact tensile tests on notched specimens made of three different types of SHCC. Two SHCC consisted of a normal-strength cementitious matrix and were reinforced with polyvinyl-alcohol (PVA) and ultra-high molecular weight polyethylene (UHMWPE) fibers, respectively. The third type consisted of a high-strength cementitious matrix and UHMWPE fibers. The dynamic tests were performed in a split Hopkinson tension bar and enabled an accurate description of the crack opening behavior in terms of force-displacement relationships at displacement rates of up to 6 m/s (19.7 ft/s).

Related References:

1. Li, V.C., 2003, “On engineered cementitious composites (ECC): A review of the material and its applications”, Journal of Advanced Concrete Technology, 1(3), 215-230.

2. Kunieda, M., Rokugo, K., 2006, “Recent progress on HPFRCC in Japan”, Journal of Advanced Concrete Technology, 4(1), 19-33.

3. Hussein, M. Kunieda, M., Nakamura, H., 2012, “Strength and ductility of RC beams strengthened with steelreinforced strain hardening cementitious composites”, Cement and Concrete Composites, 34, 1061-1066.

4. Kunieda, M., Ueda, N., Nakamura, H., Tamakoshi, T., 2013, “Cyclic response of damaged members repaired by different types of SHCCs”, In: Van Mier, J.G.M. et al. (Eds.), Proceedings of the VIII International Conference on Fracture Mechanics of Concrete and Concrete Structures FraMCoS-8, Toledo, Spain.

5. Mechtcherine, V., 2013, “Novel cement-based composites for the strengthening and repair of concrete structures”, Construction and Building Materials, 41, 365-373.

6. Kim, Y. Y., Lee, B.Y., Bang, J.W., Han, B.C., Feo, L., Cho, C.G., 2014, “Flexural performance of reinforced concrete beams strengthened with strain-hardening cementitious composites and high strength reinforcing bar”, Composites: Part B, 56, 512-519.

7. Mechtcherine, V., Silva, F.D.A., Butler, M., Zhu, D., Mobasher, B., Gao, S.-L., Mäder, E., 2011, “Behaviour of strain-hardening cement-based composites under high strain rates, Journal of Advanced Concrete Technology, 9(1), 51-62.

8. Maalej, M., Quek, S.T., Ahmed, S.F.U., Zhang, J., Lin, V.W.J., Leong, K.S., 2012, “Review of potential structural applications of hybrid fiber Engineered Cementitious Composites”, Construction and Building Materials, 36, 216-227.

9. Ranade, R., Li, V.C., Heard, W.F., 2015, “Tensile rate effects in high strength-high ductility concrete”, Cement and Concrete Research, 68, 94-104.

10. Yang, E.-H., Li, V.C., 2010, “Strain-hardening cement optimization and component tailoring by means of micromechanical model”, Construction and Building Materials, 24, 130-139.

11. Yang, E.-H., Li, V.C., 2012, “Tailoring engineered cementitious composites for impact resistance”, Cement and Concrete Research, 42(8), 1066–1071.

12. Mechtcherine, V., Millon, O., Butler, M., Thoma, K., 2011, “Mechanical behavior of strain-hardening cement-based composites under impact loading”, Cement and Concrete Composites, 33, 1–11.

13. Mechtcherine, V., Silva, F.D.A., Müller, S., Jun, P., Filho, R.D.T., 2012, “Coupled strain rate and temperature effects on the tensile behavior of strain-hardening cement-based composites (SHCC) with PVA fibers”, Cement and Concrete Research, 42, 1417–1427.

14. Yang, E.-H., Li, V.C., 2014, “Strain-rate effects on the tensile behavior of strain-hardening cementitious composites”, Construction and Building Materials, 52, 96-104.

15. Curosu, I., Mechtcherine, V., Millon, O., 2016, “Effect of fiber properties and matrix composition on the tensile behavior of strain-hardening cement-based composites (SHCCs) subject to impact loading”, Cement and Concrete Research, 82, 23-35.

16. Curosu, I., Mechtcherine, V., Forni, D., Cadoni, E., 2017, “Performance of various strain-hardening cementbased composites (SHCC) subject to uniaxial impact tensile loading”, Cement and Concrete Research, 102, 16-28.

17. Heravi, A.A., Curosu, I., Mechtcherine, V., 2020, “A gravity-driven split Hopkinson bar for investigating quasi-ductile and strain-hardening cement-based composites under tensile loading”, Cement and Concrete Research, 105, 103430.

18. Schuler, H., Mayrhofer, C., Thoma, K., 2006, “Spall experiments for the measurement of the tensile strength and fracture energy of concrete at high strain rates”, International Journal of Impact Engineering, 32, 1635-1650.

19. Reinhardt, H.W., Körmeling, H.A., Zielinsky, A.J., 1986, “The split Hopkinson bar, a versatile tool for impact testing of concrete”, Materials and Structures, 19, 55-63.

20. Gerlach, R., Kettenbeil, C., Petrinic, N., 2012, “A new split Hopkinson tensile bar design”, International Journal of Impact Engineering, 50, 63-67.

21. Xia, K., Yao., W., 2015, “Dynamic rock tests using split Hopkinson (Kolsky) bar system – A review”, Journal of Rock Mechanics and Geotechnical Engineering, 7, 27-59.

22. Cadoni, E., Forni, D., 2016, “Experimental analysis of the UHPFRCs behavior under tension at high stress rate”, The European Physical Journal Special Topics, 225(2), 253-264.

23. Kuraray Co. Ltd. (2018) Kuralon K II high tenacity type fibers. http://www.kuraray.co.jp/kii/english/ (accessed 6 July, 2018).

24. Drechsler, A., Frenzel, R., Caspari, A., Michel, S., Holzschuh, M., Synytska, A., Curosu, I., Liebscher M., Mechtcherine, V., 2019, “Surface modification of poly(vinyl alcohol) fibers to control the fiber-matrix interaction in composites”, Colloid and Polymer Science 1-15, doi: 10.1007/s00396-019-04528-z

25. Redon, C., Li, V.C., Wu, C., Hoshiro, H., Tadashi, S., Ogawa, A., 2001, “Measuring and modifying interface properties of PVA fibers in ECC matrix”, Journal of Materials in Civil Engineering, 13(6), 399-406.

26. Li, V.C., Wu, C., Wang, S., Ogawa, A., Saito, T., 2002, “Interface Tailoring for Strain-Hardening Polyvinyl Alcohol-Engineered Cementitious Composite (PVA-ECC)”, ACI Materials Journal, 99(5), 463-472.

27. Fact Sheet, Ultra High Molecular Weight Polyethylene fiber from DSM Dyneema, Eurofibers, (2012). https://issuu.com/eurofibers/docs/name8f0d44 (accessed January 9, 2020).

28. Jun, P., Mechtcherine, V., 2010, “Behaviour of Strain-hardening Cement-based Composites (SHCC) under monotonic and cyclic tensile loading, Part I – Experimental investigations”, Cement and Concrete Composites, 32, 801-809.

29. Mündecke, E., Mechtcherine, V., 2014, “Crack development in SHCC elements reinforced with steel bars and subjected to tensile loading”, In: Schlangen, E., et al. (Eds.): Proceedings of the 3rd International RILEM Conference on Strain Hardening Cementitious Composites SHCC3, Dordrecht, Netherlands, RILEM S.A.R.L.

Publications, 401-408.

30. Kamal, A., Kunieda, M., Ueda, N., Nakamura, H., 2008, “Evaluation of crack opening performance of a repair material with strain hardening behavior”, Cement and Concrete Composites, 30(10), 863-871.

31. Kanda, T., Takaine, Y., Tomoe, S., Takahashi, M., Yamamoto, Y., Kawano, K., Kunieda, M., Mizobuchi, T., 2014, Development of coupling beam elements utilizing UHP-SHCC for high-rise R/C building”, In Schlangen, E., et al. (Eds.): Proceedings of the 3rd RILEM Conference on Strain-Hardening Cementitious Composites SHCC3,

Dordrecht, Netherlands, RILEM S.A.R.L. Publications, 409-416.

32. Kolsky, H., 1949, “An investigation of the mechanical properties of materials at very high rates of loading”, Proceedings of the Physical Society Section B, 62(11), 676-700.

33. Cadoni, E., 2010, “Dynamic characterization of orthogneiss rock subjected to intermediate and high strain rates in tension”, Rock Mechanics and Rock Engineering, 43, 667-676.

34. Cadoni, E., Forni, D., Bonnet, E., Dobrusky, S., 2019, “Experimental study on direct tensile behaviour of UHPFRC under high strain-rates”, Construction and Building Materials, 218, 667-680.

35. Curosu, I., 2018, “Influence of fiber type and matrix composition on the tensile behavior of strain-hardening cement-based composites (SHCC) under impact loading”, Doctoral Thesis, Technische Universität Dresden, ISBN 978-3-86780-555-1.

36. Millon, O., Riedel, W., Thoma, K., Fehling, E., Nöldgen, M., 2009, “Fiber-reinforced ultra-high performance concrete under tensile loads”, Proceedings of the 9th International Conference on the Mechanical and Physical Behaviour of Materials Under Dynamic Loading - DYMAT, 1, 671-677.