Overview of Torsion Design Methods

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Overview of Torsion Design Methods

Author(s): Camilo Granda Valencia and Eva Lantsoght

Publication: Symposium Paper

Volume: 344

Issue:

Appears on pages(s): 1-29

Keywords: codes, concrete, reinforcement, shear, torsion

DOI: 10.14359/51728288

Date: 10/1/2020

Abstract:
Large torsional moments, which need to be considered in a design, can result among others, in structures with an asymmetric layout or loading. To find the required longitudinal and transverse reinforcement to resist these torsional moments, the link between the three-dimensional action of the torsional moment and sectional analysis methods is necessary. This paper reviews the existing methods and code provisions for torsion. First, an overview of the principles of torsion from the mechanics perspective is given. Then, a survey of the available mechanical models for torsion is presented. Finally, the code provisions for torsion of ACI 318-19, CSA-A23.3-04, AASHTO-LRFD-17, EN 1992-1-1:2004, and the fib Model Code 2010 are summarized. Additionally, current research topics on torsion in structural concrete are summarized. It is expected that with this paper, engineers will have a useful overview and background knowledge for the design and assessment of torsion-critical elements.

Related References:

1. Nilson, A., Winter, G. & Urquhart, L.1991. Design of concrete structures, McGraw-Hill., New York, NY.

2. ACI Committee 438. 1969. Tentative Recommendations for the Design of Reinforced Concrete Members to Resist Torsion, Journal of the American Concrete Institute, Proc., 66(1), 1-8.

3. ACI Committee 318. 1971. Building Code Requirements for Reinforced Concrete (ACI 318-71), Detroit, MI

4. Wight, J. 2016. Reinforced concrete: mechanics and design 7ed., Pearson Education, Inc., New Jersey, NJ

5. Collins, M.P., and Lampert, P. 1973. Redistribution of Moments at Cracking—The Key to Simpler Torsion Design?, American Concrete Institute (ACI) Special Publication (SP-35), 343-384.

6. ACI Committee 318. 2019. Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary, Farmington Hills, MI

7. Canada Standards Association. 2004. CSA-A23.3-04 Design of concrete structures, Ontario, Canada

8. American Association of Highway and Transportation Officials. 2017. AASHTO LRFD Bridge Design Specifications, 8th Edition, Washington, D.C.

9. European Committee for Standardization. 2004. Eurocode 2: Design of concrete structures - Part 1-1: General rules and rules for buildings, Brussels, Belgium

10. The International Federation for Structural Concrete. 2010. fib Model Code for Concrete Structures 2010, Lausanne, Switzerland

11. Kurrer, K. 2008. The history of the theory of structures: from arch analysis to computational mechanics, Ernst & Sohn, Berlin

12. Elfgren, L. 2009. Development of Models for Torsion of Concrete Structures in Northern Europe, American Concrete Institute (ACI) Special Publication (SP-265), 309-326.

13. Navier, C. L. 1826, “Résumé des leçons données à l'École des ponts et chaussées sur l'application de la mécanique à l'Établissement des constructions et des machines”, Première partie, “continant les leçons sur la résistance des matériaux et sur l'établissement des constructions en terre, en maçonnerie et en charpente”, Article V, “de la résistance d'un corps prismatique à la torsion”., Article VI, “de la résistance d'un corps prismatique à la ruptura causée par la torsion”, pp. 71-76, pp. 76-80, Firmin Didet, Paris.

14. Timoshenko, S. P. 1905. Lateral buckling of I-beams under the influence of forces acting in the plane of largest rigidity. In Russian. Proceedings of the St. Petersburg Polytechnic Institute, vol 4, No 3-4, 1905, pp 151-219 and vol 5, No 1-2, 1906, pp 3-34. (The writer has not seen the original paper. The reference is quoted from Timoshenko’s autobiography “As I Remember", translated from the Russian by Robert Addis, D vanNostrand, Princeton, New Jersey 1968, 430 pp.)

15. Vlasov, V. Z. 1940. Thin-walled elastic beams. English translation of the 2nd Russian edition by US Department of Commerce, Office of Technical Services, OTS 61-11400, Israel Program for Scientific Translations, Jerusalem 1961, 493 pp.

16. Elfgren, L. 1972. Reinforced Concrete Beams Loaded in Combined Torsion, Bending and Shear. A Study of the Ultimate Load-Carrying Capacity. PhD thesis, Division of Concrete Structures, Chalmers University of Technology, second edition, Göteborg, Sweden.

17. Kollbrunner, C. and Basler, K. 1969. Torsion in Structures, An Engineering Approach, Springer-Verlag Berlin Heidelberg, Berlin, Germany

18.Graf, O. and Mörsch, E, 1922, “Verdrehungsversuche zur Klärung der Schubfestigkeit von Eisenbeton. Forschungsarbeiten auf dem Gebiete des Ingenieurwesens, Heft 258, Verein Deutscher Ingenieure (VDI)”, Berlin, 52 pp.

19. Hsu, T.T.C., and Mo, Y. 1985. Softening of Concrete in Torsional Members - Theory and Tests, Journal of the American Concrete Institute, Proceedings, 82(3), 290-303.

20. Rausch, E. Design of reinforced concrete in torsion (Berechnung desEisenbetons gegen Verdrehung). Ph.D. thesis. Berlin: Technische Hochschule;1929. p. 53

21. Lessig, N. N. 1959. Determination of the Load Carrying Capacity of Reinforced Concrete Elements with Rectangular Cross-Section Subjected to Flexure with Torsion,Work 5, Institute Betona i Zhelezobetona, Moscow, pp. 4–28; also available as Foreign Literature Study 371, PCA Research and Development Labs, Skokie, IL.

22. Yudin, V. K. 1962, “Determination of the Load-Carrying Capacity of Rectangular Reinforced Concrete Elements Subjected to Combined Torsion and Bending”, Beton I Zhelezobeton (Concrete and Reinforced Concrete), No. 6, pp. 265-269 (In Russian). Translated by the Portland Cement Association , Foreign Literature Study No. 377

23. Mitchell, D., and Collins, M.P. 1974. Diagonal Compression Field Theory—A Rational Model for Structural Concrete in Pure Torsion, ACI Journal, 71(8), 396-408.

24. Hsu, T.T.C. 1988. Softening Truss Model Theory for Shear and Torsion, ACI Structural Journal, 85(6), 624-635

25. Rahal, K.N., and Collins, M. P. 2003. Combined Torsion and Bending in Reinforced and Prestressed Concrete Beams, ACI Structural Journal, 100(2), 157-165.

26. Rahal, K.N., and Collins, M.P. 1995. Analysis of Sections Subjected to Combined Shear and Torsion-A Theoretical Model, ACI Structural Journal, 92(4), 459-469.

27. Hsu, T.T.C. 1984. Torsion of reinforced concrete, Van Nostrand Reinhold Company Inc., New York, NY.

28. Ritter, W. 1899. Die Bauweise Hennebique, Schweiz Bauzeitung, 33(7), 59–61

29. Collins, M.P., and Mitchell, D. 1980. Shear and Torsion Design of Prestressed and Non-Prestressed Concrete Beams, PCI Journal, 25(4), 32-100.

30. Collins, M.P., Walsh, P.F., Archer, F.E., and Hall A.S. 1968. Ultimate Strength of Reinforced Concrete Beams Subjected to Combined Torsion and Bending, American Concrete Institute (ACI) Special Publication (SP-18), 379- 402.

31. Hsu, T.T.C. 1990. Shear flow zone in torsion of reinforced concrete, Journal of Structural Engineering ASCE, 116(11), 3206-3226.

32. Vecchio, F.J., and Collins, M.P. 1986. The Modified Compression Field Theory for Reinforced Concrete Elements Subjected to Shear. ACI Journal, Proceedings. 82(2), 219-231.

33. Bentz, E.C., Vecchio, F.J., and Collins, M.P. 2006. Simplified Modified Compression Field Theory for Calculating Shear Strength of Reinforced Concrete Elements. ACI Structural Journal, 103(4), 614-629.

34. Jeng, C.-H., and Hsu, T.T.C. 2009. A softened membrane model for torsion in reinforced concrete members, Engineering Structures, 31(9), 1944-1954.

35. Hsu, T.T.C., and Zhu, R.R.H. 2002. Softened membrane model for reinforced concrete elements in shear, ACI Structural Journal, 99(4), 460–469.

36. Völgyi, I., and Windisch, A. 2014. Resistance of reinforced concrete members with hollow circular cross-section under combined bending and shear - Part II: New calculation model. Structural Concrete, 15(1), 21–29.

37. Völgyi, I., Windisch, A., and Farkas, G. 2014. Resistance of reinforced concrete members with hollow circular cross-sections under combined bending and shear - Part I: experimental investigation, Structural Concrete, 15(1), 13–20.

38. Valdivieso, D.A., Lantsoght, E.O.L., and Sánchez, T.A. 2016. Effect of torsion on shear capacity of slabs, 6th International Conference on Structural Engineering, Mechanics and Computation: Proceedings of the 6th International Conference on Structural Engineering, Mechanics and Computation, Cape Town, South Africa, Conference Paper, 1-6

39. Lee, J-Y., Kim, K-H., Lee, S.H., Kim, C., and Kim, M-H. 2018. Maximum Torsional Reinforcement of Reinforced Concrete Beams Subjected to Pure Torsion, ACI Structural Journal, 115(3), 749-756.

40. Japan Society of Civil Engineering. 2007. Standard Specifications for Concrete Structures, Japan Society of Civil Engineering, Tokyo, Japan

41. Chiu, H.-J., Fang, I.-K., Young, W.-T., and Shiau, J.-K. 2007. Behavior of reinforced concrete beams with minimum torsional reinforcement, Engineering Structures, 29(9), 2193-2205.

42. Fang, I.-K., and Shiau, J.-K. 2004. Torsional behavior of normal- and high-strength concrete beams, ACI Structural Journal, 101(3), 304-313.

43. Shahrooz, M.B., Forry, L.M., Anderson, S.N., Bill, L.H., and Doellman M.A. 2016. Continuous Transverse Reinforcement—Behavior and Design Implications, ACI Structural Journal, 113(5), 1085-1094.

44. Koutchoukali, N., and Belarbi, A. 2001. Torsion of High-Strength Reinforced Concrete Beams and Minimum Reinforcement Requirement, ACI Structural Journal, 98(4), 462-469.

45. Mohamed, H., and Benmokrane, B. 2015. Torsion Behavior of Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars and Stirrups, ACI Structural Journal, 112(5), 543-552.

46. Yap, S.P., Khaw, K.R., Alengaram, U.J., and Jumaat, M.Z. 2015. Effect of fibre aspect ratio on the torsional behaviour of steel fibre-reinforced normal weight concrete and lightweight concrete, Engineering Structures, 101, 24-33.

47. Wafa, F.F., Hasnat, A., and Tarabolsi, O.F. 1992. Prestressed fiber-reinforced concrete beams subjected to torsion. ACI Structural Journal, 89(3), 272–83.

48. Mansur, M.A., and Lim, T.Y. 1985. Torsional behaviour of reinforced fibre concrete beams, International Journal of Cement Composites and Lightweight Concrete, 7(4), 261–267.

49. Narayanan, R., and Kareem-Palanjian, A.S. 1986. Torsion in beams reinforced with bars and fibers, Journal of Structural Engineering ASCE, 112(1), 53–66.

50. Mansur, M.A., Nagataki, S., Lee, S.H., and Oosumimoto, Y. 1989. Torsional response of reinforced fibrous concrete beams. ACI Structural Journal, 86(1), 36–44.

51. El-Niema, E.I. 1993. Fiber reinforced concrete beams under torsion. ACI Structural Journal, 90(5), 489–95.

52. Gunneswara Rao, T. D., and Rama Seshu, D. 2003. Torsion of steel fiber reinforced concrete members. Cement and Concrete Research, 33(11), 1783–1788.

53. Chalioris, C. E., & Karayannis, C.G. 2009. Effectiveness of the use of steel fibres on the torsional behaviour of flanged concrete beams, Cement and Concrete Composites, 31(5), 331-341.

54. Deifalla, A., and Ghobarah, A. 2010. Strengthening RC T-beams subjected to combined torsion and shear using FRP fabrics: Experimental study, Journal of Composites for Construction, 14(3), 301-311.

55. Chalioris, C. E. 2007. Analytical model for the torsional behaviour of reinforced concrete beams retrofitted with FRP materials, Engineering Structures, 29(12), 3263-3276.

56. He, R., Sneed, L., & Belarbi, A. 2014. Torsional Repair of Severely Damaged Column Using Carbon Fiber-Reinforced Polymer, ACI Structural Journal, 111(3), 705-716.