Title:
Mechanical characterization of fiber reinforced floor screeds: Influence of glass fibers on shrinkage and cracking mechanisms
Author(s):
Chelha, F.; Alam, S. Y.; Bendimerad, A.Z.; Loukili, A.
Publication:
Symposium Paper
Volume:
343
Issue:
Appears on pages(s):
70-79
Keywords:
Shrinkage; glass fibers; self-compacting mortar; floor screed; cracking
DOI:
Date:
10/1/2020
Abstract:
Self-compacting mortars and concretes for horizontal structures are cementitious mixtures that are both fluid and homogeneous, with the particularity of flowing under the effect of their own weight. Thanks to their homogeneous texture they offer the possibility of achieving good quality of finishing and many such advantages become the reason for their applications especially in slabs and floors. However, self-compacting mortars or concretes show considerable shrinkage and cracking problems when used in floors and slabs (Weiss et al., 1998). Because of their large moisture
exchange surfaces, the floor screeds are subjected to significant drying effects and in particular plastic shrinkage. If the movements are restrained, the risk of cracking is high. In this respect the use of fibers is a good alternative to using reinforcement bars and welded wire mesh. Indeed on site a clear decrease in cracking caused mainly by the shrinkage can be observed as soon as the fibers are incorporated in the screed. This study is conducted to demonstrate the effectiveness and the effects of glass fibers on the control of cracking phenomena due to shrinkage by determining their mechanisms of action at young age. The study is carried out in two parts: Firstly, free shrinkage behavior is analyzed in the fiber reinforced floor screed. Secondly, the restrained behavior at young ages using recently developed uni-axial tensile testing machine is investigated.
Related References:
Cortas, R. (2012). Nouvelle approche expérimentale pour la maitrise de la fissuration du béton jeune : Influence de la nature et de la saturation des granulats. PhD thesis Ecole
Centrale de Nantes and Université libre de Bruxelles.
Loukili, A. (2011). Les Bétons Auto-Plaçants (Hermes Sci).
Mangat, P. ., & AZARI, M. . (1990). Plastic shrinkage of steel fibre reinforced concrete. Materials and Structures, 23(3), 186–195.
Messan, A., Ienny, P., & Nectoux, D. (2011). Free and restrained early-age shrinkage of mortar: Influence of glass fiber, cellulose ether and EVA (ethylene-vinyl acetate). Cement
and Concrete Composites, 33(3), 402–410.
Naaman, A. E., Thanasak, W., & Hauser, G. (2005). Influence of different fibers on plastic shrinkage cracking of concrete. Aci Materials Journal, 102(1), 49–58.
Rozière, E., Granger, S., Turcry, P., & Loukili, A. (2007). Influence of paste volume on shrinkage cracking and fracture properties of self-compacting concrete. Cement and
Concrete Composites, 29(8), 626–636.
Turcry, P. (2004). Retrait et Fissuration des Betons Autoplaçants Influence de la Formulation. PhD thesis, Ecole Centrale de Nantes.
Stefan, L., Benboudjema, F.,Torrenti, J,M., Bissonnette, B. (2010). Prediction of elastic properties of cement pastes at early ages. Computational Materials Science, 47, 775-784
Weiss J. W., Yang W., Shah S. P. (1998). Shrinkage Cracking of Restrained Concrete Slabs. Journal of Engineering Mechanics, 124, 765.