Non-Linear Evaluation of Strengthening Techniques for the Champlain Bridge

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Non-Linear Evaluation of Strengthening Techniques for the Champlain Bridge

Author(s): Denis Mitchell, Bruno Massicotte, William D. Cook, and Emre Yildiz

Publication: Symposium Paper

Volume: 342

Issue:

Appears on pages(s): 143-161

Keywords: bridges, post-tensioned concrete, deterioration, flexure, shear, finite element analysis, CFRP, girders, rehabilitation

DOI: 10.14359/51725942

Date: 6/1/2020

Abstract:
The existing Champlain Bridge is a major structure in Montreal. It contains 50 concrete spans. The 10 ft (3.1 m) deep I-girders span 172 ft (52.4 m) and are post-tensioned. Because the prestressing steel has suffered from corrosion, it was necessary to use advanced techniques to evaluate the performance of these I-girders. Detailed twodimensional non-linear finite element modelling was used to determine the responses at service load and at ultimate. Three-dimensional finite element modelling was carried out to determine the loading for the two-dimensional modelling. The serviceability checks examined if cracking would occur and the strength requirements were evaluated using predicted demand-to-capacity ratios (D/C). These analysis tools also enabled the influence of a number of strengthening techniques to be assessed. The influence of different strengthening techniques on the predicted responses of the diaphragms was also studied. The combinations of strengthening measures were found to be effective in achieving the desired serviceability and strength requirements.

Related References:

Bartlett, F.M., and MacGregor, J.G. 1995. “Equivalent Specified Concrete Strength from Core Test Data.” Concrete International, Vol. 17, No. 3, pp. 52–58.

Bentz, E.C. and Collins, M.P. 2015. http://www.ecf.utoronto.ca/~bentz/r2k.htm, Response-2000 webpage last accessed 2015/02/13.

CSA, 2014, CSA S6-14. 2014. “Canadian Highway Bridge Design Code”, Canadian Standards Association, Mississauga, ON.

Hibbitt, Karlsson, and Sorensen. 2014. ABAQUS/Explicit user's Manual version 6.14-2.

JCCBI. 1998. « Pont Champlain, Sections 5 & 7 Réfection de 8 Poutres de Béton (1998) – Détails de Renforcement des Poutres par Post-Tension », No. Contrat 92-40-8767, No. Dessin 125101-06.

JCCBI. 2011. « Pont Champlain, Sections 4, 5 and 6, réfection des piles, chevêtres, poutres et joints de tablier (2012-2013) », AECOM, Contrat no. 61579, dessins 125570.

JCCBI. 2013. « Champlain Bridge, Section 5, Rehabilitation of Piers, Beams, Slab and Deck Joints – Beams Strengthened with Additional Post-Tensioning, Dessau, drawing 125728 – 402.

Vecchio, F.J. 2017. http://www.civ.utoronto.ca/vector, VecTor2 webpage, last accessed 2017/09/13.

Warycha, L. and Skotecky, C. 1960. “Champlain Bridge Sections 5 and 7A – Transverse Cabling and Reinforcing”, JCCBI Drawing 12942-EE-26.

Warycha, L. and Skotecky, C. 1960. “Construction of Piers and Superstructure - Section 5 and 7A of Champlain Bridge – I Explanatory Note – Calculation and References”, revised April 1960, JCCBI Document 0277.