Title: ACI 515.3R-20 Guide for Assessment and Surface Preparation for Application of Protection Systems for Concrete
Author(s): ACI Committee 515
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 20
Keywords: coatings; membranes; protection systems; surface preparation.
DOI:
Date: 5/22/2020
Abstract: This document provides general guidance for determining appropriate acceptance criteria for a prepared surface to receive a protection system. There are many techniques for preparation of a surface prior to installation of a protection system, and no single method is ideal for all situations. This guide discusses various preparation methods that can be used to achieve the intended surface condition.
ACI Collection of Concrete Codes, Specifications, and Practices - Digital Subscription
ACI 562 PLUS Concrete Repair Subscription
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Edit Module Settings to define Page Content Reviewer