SP-339-12: Interaction of Sliding, Shear, and Flexure for Earthquake Design of Reinforced Concrete Shear Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: SP-339-12: Interaction of Sliding, Shear, and Flexure for Earthquake Design of Reinforced Concrete Shear Walls

Author(s): Burkhart Trost, Harald Schuler, and Bozidar Stojadinovic

Publication: Symposium Paper

Volume: 339

Issue:

Appears on pages(s): 196-216

Keywords: sliding, shear walls, crack, flexural crack, cold joint, friction, aggregate interlock, pushover

DOI: 10.14359/51724703

Date: 3/1/2020

Abstract:
Sliding failure of reinforced concrete shear walls was observed after the Chilean earthquakes in 1985 and 2010, during shaking table tests, and in many quasi-static cyclic shear walls tests. Sliding may occur along cold joints or flexural cracks that remain open due to permanent deformations induced during cyclic loading. If it occurs, sliding can significantly reduce the horizontal force resistance and change the deformation mechanism of reinforced concrete shear walls, and thereby markedly affect the seismic performance of shear wall buildings. This study provides the interaction diagrams intended to help reinforced concrete shear wall designers exclude the sliding failure mode. Regions where sliding, shear, and flexural failure modes are expected are delineated according to the shear wall shear span to length ratio, the axial force, the horizontal and vertical reinforcement ratios, and the concrete strength. These interaction diagrams are derived using a cyclic reinforced concrete wall response model that considers flexure, shear and sliding load-deformation relationships and the interaction between them. The inter-action diagram is used to develop design recommendations on how to avoid the sliding failure of reinforced concrete shear walls under earthquake loading.

Related References:

1. Earthquake Engineering Research Institut, “The Chile Earthquake of March 3, 1985: Performance of Structures,” Earthquake Spectra, 2-2, 1986, pp. 293–371.

2. Sherstobitoff, J., Cajiao, P., and Adebar, P., “Repair of an 18-Story Shear Wall Building Damaged in the 2010 Chile Earthquake,” Earthquake Spectra, V. 28, 28-1, 2012, pp. 335–348.

3. Nagae, T., Ghannoum, W. M., Kwon, J., Tahara, K., Fukuyama, K., Matsumori, T., Shiohara, H., Kabeyasawa, T., Kono, S., Nishiyama, M., Sause, R., Wallace, J. W., and Moehle, J. P., “Design Implications of Large-Scale Shaking Table Test on Four-Story Reinforced Concrete Building,” ACI Structural Journal, 112-2, 2015, pp. 135–146.

4. Synge, A. J., “Ductility of squat shear walls,” Research Report, University of Canterbury, Department of Civil Engineering, Christchurch, 1980, 142 pp.

5. Wasiewicz, Z. F., “Sliding shear in low rise shear walls under lateral load reversals,” Master thesis, University of Ottawa, Department of Engineering, Ottawa, 1988, 152 pp.

6. Greifenhagen, C., “Seismic behavior of lightly reinforced concrete squat shear walls,” Lusannne, 2006.

7. Salonikios, T. N., Kappos, A. J., Tegos, I. A., and Penelis, G. G., “Cyclic Load Behavior of Low-slenderness Reinforced Concrete Walls: Design Basis and Test Results,” ACI Structural Journal, 96-4, 1999, pp. 649–660.

8. Wiradinata, S., “Behaviour of squat walls subjected to load reversals,” Master thesis, University of Toronto, Department of Civil Engineering, Toronto, 1985.

9. Whyte, C. A., and Stojadinovic, B., “Hybrid Simulation of the Seismic Response of Squat Reinforced Con-crete Shear Walls,” Berkeley, California, 2013, 221 pp.

10. Luna, B., Rivera, J., Rocks, J., goksu, C., Weinreber, S., and Whittaker, A., “Low Aspect Ratio Rectangular Reinforced Concrete Shear Wall: Specimen SW8,” 2013.

11. Trost, B., Schuler, H., and Stojadinovic, B., “Sliding deformation model for reinforced concrete shear walls under seismic loading,” Proceedings of the 16th World Conference on Earthquake Engineering, 2017.

12. 2004, Eurocode 2 : Design of Concrete Structures - Part 1-1: General rules and rules for buildings, European Commitee for Standardiasation, Brussels, EN 1992-1-1.

13. “CEB-FIP Model Code 1990: Design Code,” Thomas Telford, London, 1993, 437 pp.

14. Alvarez, M., Marti, P., Sigrist, V., and Kaufmann, W., “Tragverhalten von Stahlbeton: Fortbildungskurs für Bauingenieure,” 1999.

15. Muttoni, A., “Die Anwendbarkeit der Plastizitätstheorie in der Bemessung von Stahlbeton,” Birkhäuser Basel, Basel, 1990, 158 pp.

16. Trost, B., Schuler, H., and Stojadinovic, B., “Sliding in the compression zone of reinforced concrete shear walls: Behavior and Modeling” ACI Structural Journal, 116-5, 2019, pp. 3-16.

17. Trost, B., “Interaction of sliding, shear and flexure in the seismic response of squat reinforced concrete shear walls,” Zurich, 2017.

18. Luna, B. N., Rivera, J. P., and Whittaker, A. S., “Seismic Behavior of Low-Aspect-Ratio Reinforced Concrete Shear Walls,” ACI Structural Journal, 112-5, 2015, pp. 593–604.

19. Deutsches Institut für Normung, Concrete, reinforced and prestressed concrete structures: Part 2: Concrete - Specification, properties, production and conformity - Application rules for DIN EN 206-1, Beuth, Berlin, DIN 1045-2.