Title:
Concrete Mix Design Development for Offshore Structures
Author(s):
Kjell Tore Fosså and Widianto
Publication:
Symposium Paper
Volume:
337
Issue:
Appears on pages(s):
78-88
Keywords:
Gravity Based Structure, Concrete Mix, Slipforming, Offshore, Aggregate, High-Strength, Cement, Admixtures, Pozzolans
DOI:
10.14359/51724548
Date:
1/23/2020
Abstract:
This paper describes the development in concrete technology for offshore concrete structures from the 1970’s until now and discusses some potential topics for future research which would result in more cost-effective
offshore concrete structures.
Most of the offshore concrete structures constructed in the last 4 decades are still in operation, with no or only minor maintenance required, even though the average age for these structures in the North Sea is more than 25 years. The compressive strength in offshore structures has gradually increased from about 40MPa (5800 psi) in the 1970’s to more than 100MPa (14500 psi) in some of the latest concrete structures. Standards and concrete specifications have been revised several times during these years. In parallel, the knowledge from several research and development programs has been used to further improve the concrete properties and overcome the limitations. Focus has been primarily to improve the compressive strength of the concrete as well as the durability and concrete
workability. The cement and admixture industry have been heavily involved in research programs to further adapt and develop these material properties. The result of the product developments in the concrete constituency has also improved cost-effectiveness and durability (including overall life-cycle cost-effectiveness) for offshore concrete structures.
With the new generation technology, the technical limitations we face today will be overcome. With more knowledge and improved technology, the quantity and size of cracks in concrete in service are expected to be reduced, which would also improve durability. In addition, the focus in the future will also be on sustainable and environmentally friendly materials.
Related References:
1. Fib Report, Bulletin 50, 2009, “Concrete Structures for Gas and Oil Field in Hostile Marine Environments”.
2. Widianto, Jameel Khalifa, Erik Åldstedt, Kåre O. Hæreid, Kjell Tore Fosså. 2020. Design and Construction Overview of Offshore Concrete Gravity-Based-Structure: Past, Present, and Future. ACI Special Publication, ACI.
3. NS 3473 E, 1993, “Design of Concrete Structures, Design and detailing rules”.
4. Jacobsen, S. (editor), 2016, “Concrete Technology” NTNU, Department of Structural Science, Trondheim Norway.
5. Second International Symposium on Structural Lightweight Aggregate Concrete, 18-22 June 2000, Kristiansand, Norway
6. FiP Manual of Lightweight Aggregate Concrete, 2nd edition, ISBN 0-903384-43-4, Great Britain 1983.
7. Ramachandran, V.S., 1995, “Concrete Admixture Handbook- Properties, Science and Technology”, Second edition, ISBN 0-8155-1373-9, Noyes Publication, USA.
8. Norwegian annex to EN-NS 206-1” Part 1: Specification, performance, production and conformity”
9. ASTM C666, 2015, “Standard Test Method for Resistance of Concrete to Rapid Freezing and Thawing”.
10. NB-publication 25, 2018, “Guidelines for Design and Construction of Slipformed Concrete Structures”, A publication from Norwegian Concrete Society, Oslo.
11. Lorcenis – Long lasting Reinforced Concrete Structures for Energy Infrastructures under Severe Operating Conditions, EC-research program in Horizon 2020, https://www.sintef.no/projectweb/lorcenis/objectives/.
12. Fosså, K.T., 2015, “Slipforming of High Strength Concrete”, Concrete – Innovation and Design, fib Symposium, Copenhagen.
13. Fosså, K.T., 2001, “Slipforming of vertical Concrete Structures, Friction between Concrete and Slipform Panel”, PhD-dissertation, ISBN, 82-471-5325-4, Department of Structural Engineering, NTNU, Trondheim.