Title:
Rational Fuzzy Logic Condition Rating Model of Reinforced Concrete Bridge Decks Using Non-destructive Testing and Visual Inspection
Author(s):
Tarek Omar and Moncef L. Nehdi
Publication:
Symposium Paper
Volume:
333
Issue:
Appears on pages(s):
159-174
Keywords:
bridge deck, condition rating, fuzzy logic, ground penetrating radar, infrared thermography, uncertainty, visual inspection
DOI:
10.14359/51720275
Date:
10/1/2019
Abstract:
Bridge deck condition rating systems commonly use measurements of obvious defects recorded through visual investigation. Accordingly, the condition of bridge decks is rated linguistically with inherent vagueness in the description of the deck condition. Although several advanced non-destructive testing (NDT) technologies have emerged for inspecting bridge decks, their results have yet to be incorporated in the condition rating process. The present study establishes a unique link between NDT technologies and inspector findings by developing a novel bridge deck condition rating index (BDCI). The proposed procedure captures the integrated results of infrared thermography (IRT) and ground-penetrating radar (GPR), along with visual inspection judgement deployed to evaluate a full-scale aging concrete bridge deck. The information sought to identify the parameters affecting the integration process was gathered from bridge engineers with extensive experience and intuition. The analysis
process utilized the fuzzy set theory, thus overcoming the inherent scientific uncertainties and imprecision in the
measurements of bridge deck subsurface defects by IRT and GPR testing along with surface defects identified through bridge inspector observations. Integrating the proposed BDCI procedure with existing bridge management systems can provide a detailed and reliable appraisal of bridge health, thus helping transportation agencies in optimizing budgets and prioritizing maintenance, repair, and rehabilitation efforts.
Related References:
1. Maser, K., Martino, N., Doughty, J. and Birken, R., 2012, “Understanding and Detecting Bridge Deck Deterioration Using Ground Penetrating Radar.” J. Transportation Research Record. 2313: 116-123.
2. Omar, T., Nehdi, M., Zayed, T., 2017, “Rational Condition Assessment of Reinforced Concrete Bridge Decks Subjected to Corrosion-Induced Delamination.” Journal of Materials in Civil Engineering, doi: 10.1061/(ASCE)MT.1943-5533.0002114
3. Omar, T., and Nehdi, M., 2017, “Unmanned Aerial Vehicle Infrared Thermography Remote Sensing for Condition Assessment of Concrete Bridge Decks.” Automation in Construction. 83:360-371. doi: 10.1016/j.autcon.2017.06.024
4. Nasrollahi, M., and Washer, G., 2014, “Estimating Inspection Intervals for Bridges Based on Statistical Analysis of National Bridge Inventory Data.” Journal of Bridge Engineering, doi: 10.1061/(ASCE)BE.1943-5592.0000710
5. Gucunski, N., Kee, S., La, H., Basily, B., Maher, A., and Ghasemi, H., 2015, “Implementation of a Fully Autonomous Platform for Assessment of Concrete Bridge Decks.” Proc., Str. Congress, Portland, Oregon, pp: 367-378.
6. Wang, Y. and Elhag, T., 2008, “Evidential reasoning approach for bridge condition assessment.” Expert Systems with Applications, doi: 10.1016/j.eswa.2006.10.006
7. Gucunski, N., and Nazarian, S., 2010, “Material Characterization and Condition Assessment of Reinforced Concrete Bridge Decks by Complementary NDE Technologies.” Proc., Str. Congress, Orlando, Florida, United States, pp: 429-439.
8. Yehia. S., Abudayyeh, O., Nabulsi, S., and Abdel-Qader, I., 2007, “Detection of Common Defects in Concrete Bridge Decks Using NDE Techniques.” Journal of Bridge Eng.ineering, 12:2, 215-225. doi: 10.1061/(ASCE)1084-0702(2007)
9. Gucunski, N., Imani, A., Romero, F., Nazarian, S., Yuan, D., Wiggenhauser, H., Shokouhi, P., Taffe, A., and Kutrubes, D., 2013, “Non-destructive testing to identify concrete bridge deck deterioration.” Proc., 92nd Annual Meeting, TRB, Washington, D.C. SHRP 2, Report, 96 p.
10. Robert, M., 1982, “Science behind Thermography-Thermal Infrared Sensing for Diagnostics and Control.” Proc., SPIE 0371, Thermosense V. Editor: George E. Courville, doi: 10.1117/12.934450
11. ASTM Standard D4788-03, 2013, Standard Test Method for Detecting Delaminations in Bridge Decks Using Infrared Thermography, ASTM International, West Conshohocken, PA.
12. Barnes, C., Trottier, J., and Forgeron, D., 2008, “Improved Concrete Bridge Deck Evaluation Using GPR by Accounting for Signal Depth-Amplitude Effects.” J. NDT & E. Intern., doi: 10.1016/j.ndteint.2008.03.005
13. Alani, A., Aboutalebi, M., and Kilic, G., 2013, "Applications of ground penetrating radar (GPR) in bridge deck monitoring and assessment." J. Application Geophysics, doi: 10.1016/j.jappgeo.2013.04.009
14. ASTM D6087-08, 2010, Standard Test Method for Evaluating Asphalt-Covered Concrete Bridge Decks Using Ground Penetrating Radar, ASTM International, West Conshohocken, PA.
15. Bektas, B., Carriquiry, A., and Smadi, O., 2013, “Using Classification Trees for Predicting National Bridge Inventory Condition Ratings.” J. Infrastructure Systems, doi: 10.1061/(ASCE)IS.1943-555X.0000143
16. FHWA (Federal Highway Administration), 1995, Recording and coding guide for the structure inventory and appraisal of the nation’s bridges, FHWA-PD-96-001, U.S. Dept. of Transportation, Washington, DC.
17. Thompson, P., and Shepard, R., 2000, “AASHTO commonly recognized bridge elements, successful applications and lessons learned.” Prepared for the National Workshop on Commonly Recognized Measures for Maintenance. Paul D. Thompson Consultant, 1-13.
18. Kishk, M., and Al-Hajj, A., 2002, “A fuzzy model and algorithm to handle subjectivity in life-cycle costing based decision-making.” J. Financial Management and Property Constr., 5 :1-2: 93–104.
19. Ross, J., 2010, Fuzzy Logic with Engineering Applications, 3rd Edition, John Wiley and Sons Ltd, UK, 707 p. 20. Zadeh, L., 1965, “Probability theory and fuzzy logic are complementary rather than competitive.” Technometrics, 37:3, 271–276.
21. Sasmal, S., and Ramanjaneyulu, K., 2009, “Condition evaluation of existing RC bridges using FAH approach.” Expert Systems with Applications, doi: 10.1016/j.eswa.2007.08.017
22. Tee, B., Bowman, D., and Sinha, C., 1988, “A fuzzy mathematical approach for bridge condition evaluation.” J. Civil Engineering Systems, 5:1, 17-25.
23. Liang, T., Chang, W., and Li, F., 2002, “Grey and regression models predicting the remaining service life of existing RC bridges.” Grey Systems, 14:4: 291–310.
24. Li, Q., and Wang, K., 2011, “Pavement Smoothness Prediction Based on Fuzzy and Gray Theories.” Computer-Aided Civil and Infrastructure Engineering, doi: 10.1111/j.1467-8667.2009.00639.x
25. Moufti, S., Zayed, T., and Abu Dabous, S., 2014, “Defect Based Condition Assessment of Concrete Bridges: A Fuzzy Hierarchical Evidential Reasoning Approach.” Proc., Transportation Research Record, 93rd Annual Meeting, 88-96.
26. Saaty TL. 1980. The analytic hierarchy process. New York: McGraw-Hill; 20–25.
27. Zhou, X., 2012, Fuzzy Analytical Network Process Implementation with Matlab. MATLAB - A Fundamental Tool for Scientific Computing and Engineering Applications – Vol. 3, Edited by Vasilios N. Katsikis, Open Access, Chapter 6, 133-160.
28. Mikhailov, L., 2004, “Group prioritization in the AHP by fuzzy preference programming method.” J. Comput. Oper. Res., 31:2: 293–301.