A Numerical Analysis Methodology for the Strengthening of Deep Cap Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A Numerical Analysis Methodology for the Strengthening of Deep Cap Beams

Author(s): Rafael A. Salgado, Serhan Guner

Publication: Symposium Paper

Volume: 333

Issue:

Appears on pages(s): 1-18

Keywords: deep beams; nonlinear analysis; cap beam; structural assessment; FRP; retrofit; analysis methodology

DOI: 10.14359/51720267

Date: 10/1/2019

Abstract:
A significant number of in-service bridges have been subjected to loads above their original design capacities due to the increase in traffic and transported freight in the past decades. Externally bonded fiber-reinforced polymers (FRP) is a non-destructive retrofit technique that has become common for the strengthening of overloaded cap beams of bridges. However, there is a lack of analysis methods for the retrofitted cap beams that can accurately predict the retrofitted structural response while accounting for the critical material behaviors such as bond-slip relationships, confinement effects, and redistribution of stresses. In this study, an analysis methodology using nonlinear finite element models is proposed for cap beams retrofitted with externally bonded FRP fabrics. A two-stage verification of the proposed methodology was employed: a constitutive modeling and critical behavior of materials verification using experimental results available in the literature; and a system-level load capacity determination using a large, in-situ structure. The proposed methodology was able to capture the FRP-concrete composite structural behavior and the experimentally observed failure modes. The FRP retrofit layout created using the results of this study increased the capacity of the initially overloaded cap beam in 27%, granting it a 6% extra capacity under its ultimate loading condition.

Related References:

1. American Concrete Institute, “Guide for the Design and Construction of Structural Concrete Reinforced with FRP Bars (ACI 440.1R-15),” American Concrete Institute (ACI), Farmington Hills, MI, 2015, 88 pp.

2. Canadian Standards Association / National Standard of Canada, “Canadian Highway Bridge Design Code (CAN/CSA S6-14),” 11th ed., CSA Group, Mississauga, Ontario, Canada, 2014, 894 pp.

3. American Concrete Institute, “Building Code Requirements for Structural Concrete and Commentary (ACI 318-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

4. Canadian Standards Association, “Design of Concrete Structures (CSA A23.3-14),” 6th ed., CSA Group, Mississauga, Ontario, Canada, 2014, 290 pp.

5. Guner, S.; Vecchio, F. J., “Pushover Analysis of Shear-Critical Frames: Formulation,” ACI Structural Journal, V. 107, No. 1, 2010, 63-71 pp., http://www.utoledo.edu/engineering/faculty/serhan-guner/docs/JP1-Guner and Vecchio.pdf.

6. Guner, S.; Vecchio, F. J., “Pushover Analysis of Shear-Critical Frames: Verification and Application,” ACI Structural Journal, V. 107, No. 1, 2010, 72-81 pp., http://www.utoledo.edu/engineering/faculty/serhanguner/docs/JP2_Guner_Vecchio_2010b.pdf.

7. Wong, P. S.; Vecchio, F. J.; Trommels, H., “Vector2 & Formworks User’s Manual,” 2nd ed., 318 pp., http://www.vectoranalysisgroup.com/user_manuals/manual1.pdf.

8. Vecchio, F. J., “Disturbed Stress Field Model for Reinforced Concrete: Formulation,” Journal of Structural Engineering, V. September, 2000, 1070-1077 pp.,

http://www.vectoranalysisgroup.com/journal_publications/jp34.pdf.

9. Vecchio, F. J.; Collins, M. P., “The Modified Compression-Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal, V. 83, No. 2, 1986, 219-231 pp., http://www.vectoranalysisgroup.com/journal_publications/jp2.pdf.

10. American Association of State Highway and Transportation Officials. “AASHTO LRFD Bridge Design Specifications,” 4th ed., American Association of State Highway and Transportation Officials, Washington, DC, 2017, 566 pp.

11. Hognestad, E., “A Study of Combined Bending and Axial Load in Reinforced Concrete Members,” Bulletin Series No 399, 1951, 128 pp., https://www.ideals.illinois.edu/handle/2142/4360%0Ahttp://hdl.handle.net/2142/4360.

12. Coulomb, C. A., “Essai Sur Une Application des Regles de Maximis et Minimis a Quelques Problemes de Statique Relatifs a l’Architecture (Essay on Maximums and Minimums of Rules to Some Static Problems Relating to Architecture),” Memoires De La Mathematique Et De Physique, V. 7, 1973, 343–387 pp.

13. Bunni, N. G.; Scott, B.; Park, R.; Priestley, M., “Stress-Strain Behavior of Concrete Confined by Overlapping Hoops at Low and High Strain Rates,” ACI Journal, V. 79, No. 6, 1982, 496-498 pp.

14. Vecchio, F. J., “Analysis of Shear-Critical Reinforced Concrete Beams,” ACI Structural Journal, V. 97, No. 1, 2000, 102-110 pp.

15. Vecchio, F. J., “Finite Element Modeling of Concrete Expansion and Confinement,” Journal of Structural Engineering, V. 118, No. 9, 1992, 2390-2406 pp.

16. Bentz, E. C., “Explaining the Riddle of Tension Stiffening Models for Shear Panel Experiments,” Journal of Structural Engineering, V.131, No. 9, 2005, 1422-1425 pp., http://ascelibrary.org/doi/10.1061/%28ASCE%290733-9445%282005%29131%3A9%281422%29.

17. Walraven, J. C.; Reinhardt, H. W., “Theory and Experiments on the Mechanical Behaviour of Cracks in Plain and Reinforced Concrete Subjected to Shear Loading,” Heron, V. 26, No. 1A, 1981, https://repository.tudelft.nl/islandora/object/uuid:3d68bd1a-465d-4590-b33c-7ede99bbc251/datastream/OBJ/download.

18. Seckin, M., “Hysteretic Behavior of Cast-In-Place Exterior Beam-Column-Slab Assemblies,” Ph.D. Thesis, University of Toronto, Toronto, Canada, 1982.

19. Kupfer, H.; Hilsdorf, H., “Behavior of Concrete Under Biaxial Stresses,” ACI Journal, V. 66, No. 8, 1969, 656-666 pp., http://www.academia.edu/download/33736623/kupfer.pdf.

20. Richart, F.; Brandtzaeg, A.; Brown, R. L., “A Study of the Failure of Concrete under Combined Compressive Stresses,” University of Illinois Bulletin. V. 26, Bullet(12), 1928, 104 pp., http://www.academia.edu/download/33736623/kupfer.pdf.

21. He, X. G.; Kwan, A. K. H., “Modeling Dowel Action of Reinforcement Bars for Finite Element Analysis of Concrete Structures,” Computers and Structures, V. 79, No. 6, 2001, 595-604 pp.

22. Dhakal, R. P; Maekawa, K., “Modeling for Postyield Buckling of Reinforcement,” Journal of Structural Engineering, V. 128, No. 9, 2002, 1139-1147 pp., http://ascelibrary.org/doi/10.1061/%28ASCE%290733-9445%282002%29128%3A9%281139%29.

23. Dhakal, R. P.; Maekawa, K., “Reinforcement Stability and Fracture of Cover Concrete in Reinforced Concrete Members,” Journal of Structural Engineering, V. 128, No. 10, 2002, 1253-1262 pp.

24. Grelle, S. V; Sneed, L .H., “Review of Anchorage Systems for Externally Bonded FRP Laminates,” International Journal of Concrete Structures and Materials, V. 7, No. 1, 2013, 17-33 pp.

25. Sato, Y.; Vecchio, F. J., “Tension Stiffening and Crack Formation in Reinforced Concrete Members with Fiber-Reinforced Polymer Sheets,” Journal of Structural Engineering, V. 129, No. 6, 2003, 717-724 pp.

26. Wong, R. S.; Vecchio, F. J., “Towards Modeling of Reinforced Concrete Members with Externally Bonded Fiber-Reinforced Polymer Composites,” ACI Structural Journal, V. 100, No. 6, 2003, 47-55 pp., http://www.vectoranalysisgroup.com/journal_publications/jp45.pdf.

27. Ceroni, F.; Pecce, M.; Matthys, S.; Taerwe, L., “Debonding Strength and Anchorage Devices for Reinforced Concrete Elements Strengthened with FRP Sheets,” Composites Part B: Engineering, V. 39, No. 3, 2008, 429-441 pp., doi:10.1016/j.compositesb.2007.05.002

28. Cervenka, V., “Global Safety Format for Nonlinear Calculation of Reinforced Concrete,” Beton- und Stahlbetonbau, V. 103, No. S1, 2008, 37-42 pp., http://doi.wiley.com/10.1002/best.200810117.

29. Sangiorno, F., “Safety Format for Non-linear Analysis of RC Structures Subjected to Multiple Failure Modes,” Ph.D. Thesis, KTH Royal Institute of Technology, Stockholm, Sweden. 2015, 45pp.

30. European Committee for Standardization. Eurocode 2 - Design of Concrete Structures - Concrete Bridges - Design and Detailing Rules (EN 1992-2:2005). European Committee for Standardization (CEN), 2005, 95 pp.

31. Khalifa, A.; Nanni, A., “Rehabilitation of Rectangular Supported RC Beams with Deficiencies Using CFRP Composites,” Construction and Building Materials, V. 16, No. 3, 2002, 135-146 pp.

32. Al-Tamimi, A. K.; Hawileh, R.; Abdalla, J.; Rasheed, H. A., “Effects of Ratio of CFRP Plate Length to Shear Span and End Anchorage on Flexural Behavior of SCC RC Beams,” Journal of Composites for Construction, V. 15, No. 6, 2011, 908-919 pp.