Title:
Responsibility in Evaluating and Repairing Existing Concrete Structures: An Environmental Structure Case Study
Author(s):
Pericles C. Stivaros
Publication:
Symposium Paper
Volume:
332
Issue:
Appears on pages(s):
8-22
Keywords:
concrete repair, responsibility, quality control, quality assurance, structural assessment, structural evaluation, nondestructive testing
DOI:
10.14359/51719121
Date:
7/1/2019
Abstract:
A successful concrete repair project requires a close coordination of efforts between the three major parties involved: the owner, the licensed design professional (LDP), and the contractor. Lack of coordination and clear understanding of the professional and contractual responsibilities, as well as the expectations, of each party involved in a concrete repair project, could result in long legal disputes to attempt to sort out the responsibilities of each party. The greatest victim of the dispute is usually the structure itself. The American Concrete Institute (ACI) has led the effort to
develop responsibility guidelines in concrete construction. ACI 132 identifies and suggests the allocation of responsibilities to various parties involved in concrete construction. ACI 132 document is applicable to general concrete construction, and it does not consider the particularities of evaluating and repairing existing concrete structures. ACI 562 provides minimum requirements for assessment, repair and rehabilitation of existing distressed concrete structures, including a discussion on the responsibilities of the licensed design professional for the evaluation and repair of concrete structures. This paper discusses the responsibilities of the licensed design professional, the contractor, and the owner through a repair case study. The paper demonstrates the need to expand ACI 132 and/or ACI 562 to include responsibility guidelines for concrete repair projects.
Related References:
1. Quality in the Construction Project, A Guide for Owners, Designers, and Constructors,” ASCE, Third Edition,2012, 302 pp.
2. ACI Committee 132 “Guide for Responsibility in Concrete Construction (ACI 132R-14),” American Concrete Institute, Farmington Hills, Michigan, 2014, 11 pp.
3. ACI Committee 562 “Code Requirements for Evaluation, Repair, and Rehabilitation of Existing Concrete Structures and Commentary (ACI 562-16)” American Concrete Institute, Farmington Hills, Michigan, 2016, 86 pp.
4. ACI Committee 364 “Guide for Evaluation of Concrete Structures before Rehabilitation (ACI 364.1R-07),” American Concrete Institute, Farmington Hills, Michigan, 2007, 18 pp.
5. ACI Committee 350 “Code Requirements for Environmental Engineering Concrete Structures and Commentary (ACI 350-06)”, American Concrete Institute, Farmington Hills, Michigan, 2006, 485 pp.
6. ACI Committee 201 “Guide for Conducting Visual Inspection of Concrete in Service (ACI 201.1R-08),” American Concrete Institute, Farmington Hills, Michigan, 2008, 15 pp.
7. ACI Committee 224. “Causes, Evaluation and Repair of Cracks in Concrete (ACI 224.1R-07),” American Concrete Institute, Farmington Hills, Michigan, 2007, 22 pp.
8. ACI Committee 228 “Report on Nondestructive Test Methods for Evaluation of Concrete Structures (ACI 228.2R-13),” American Concrete Institute, Farmington Hills, Michigan, 2013, 82 pp.
9. ACI Committee 546R “Guide to Concrete Repair (ACI 546R-14),” American Concrete Institute, Farmington Hills, Michigan, 2014, 70 pp.
10. ICRI No. 210.4 Guide for Nondestructive Evaluation Methods for Condition Assessment, Repair, and Performance Monitoring of Concrete Structures
11. ICRI No. 310.1R Guide for Surface Preparation for the Repair of Deteriorated Concrete Resulting from Reinforcing Steel Corrosion