Behavior and Design of High-Strength RC Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior and Design of High-Strength RC Walls

Author(s): J.W. Wallace

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s): 259-280

Keywords: Earthquake-resistant structures; high-strength concrete; reinforced concrete; shear properties; strength; walls

DOI:

Date: 10/1/1998

Abstract:
Use of high-strength reinforced concrete walls in regions of high seismic risk is evaluated using current U.S. code provisions, an example building, parametric studies, and experimental results. The format of current U.S. code provisions for structural walls promotes the use of high-strength concrete; however, the use of these provisions has not been evaluated for high-strength concrete. Analytical studies of building systems utilizing slender walls indicate that there is not a significant advantage associated with the use of high-strength concrete waUs and that this advantage tends to diminish with increasing concrete strength. Evaluation of test results conducted in Japan for low-aspect ratio walls indicates that ACI 318-95 requirements do not represent the observed shear strength well. Based on the limited database considered in this study, a value of 1.0 f' c MPa (126) was found to provide a good estimate of wall shear strength.




  